Nitric acid alternative for dissolving gold?

I was ordering some more sodium nitrate online today and ran across this page on their site claiming that this product can replace the Nitric Acid in an aqua regia process (still need HCl though I think). Any thoughts?:

https://www.ishor.com/mx3-dissolving-agent
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #2  
Old 09-09-2019, 03:59 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,268
Pete VanderLaan is on a distinguished road
I can certainly see that the sodium nitrate would make an acid which would be attached to a base. HnO3 would be the regular acid but I assume this would make up some sort of NO3 that would have inclusive sodium, not something I'm sure if I would want.

It is a pain to get the nitric delivered these days. Ultimately, I got it from Graingers.

But you go first...
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 09-10-2019, 07:59 PM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 722
Josh Bernbaum is on a distinguished road
When it was delivered, I had to sign some form for the Nitric I ordered a while back. No doubt I'm on some sort of list now that I've had that and CdS and K dichromate shipped to my house over the years. But since our EPA have been instructed to promote extra pollution these days, maybe I don't need to worry. That mostly full bottle of Nitric does make me nervous though..
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #4  
Old 11-23-2019, 12:07 PM
Bradley Howes Bradley Howes is offline
Registered User
 
Join Date: Mar 2015
Location: Alfred University
Posts: 62
Bradley Howes is on a distinguished road
There's always sodium cyanide...
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 06:15 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.