Iron Sulphide glasses?

Haven't posted in a while on this batching and color forum but still glad it's here..
So lately I've been pulling quite a bit of cane with Gaffer's "Durissimo Black", pulling again in murrini and then using that in my pieces. It's a steep learning curve to using the stuff, it's SO stiff, it barely feels like glass. I've got a pretty good handle on it now though. It's taken me a while but with some adaptations in process the pulls are now finally feeling almost (almost) like cane pulls with normal duro color in the core.

I'm going to be asking John a lot of questions at the class at Penland next month, but just curious if anyone here knows some more about the chemistry. I've heard that this stuff is an Iron Sulphide glass (or Iron sulfate?). I'm not sure if that's correct or not, but I do detect a sulphur-ish smell coming off of the chunks of the bar when I'm working with it. More specifically, it's not just that it smells when it's hot, but more so when I quench parts of it after heating. Even the water in which it's quenched smells afterward. Curious about what's happening here..
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #2  
Old 03-15-2019, 01:26 AM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,698
Jordan Kube is on a distinguished road
You can melt this yourself. Not as stiff.

http://talk.craftweb.com/showthread.php?t=11375
__________________
WWUD? Think for yourself.
Reply With Quote
  #3  
Old 03-15-2019, 08:49 AM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 650
Josh Bernbaum is on a distinguished road
Do you think there's rosin in Gaffer's version Jordan?
I'm also too worried to put sulphur in my furnace here, worried about lingering smells that is.. Even the selenium I've put in melts before seemed to linger afterward.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #4  
Old 03-15-2019, 09:15 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,506
Pete VanderLaan is on a distinguished road
sulfur certainly sticks around. In a reducing atmosphere it smells for a long time. Rosin is not a requisite in a glass like this if you want the beer bottle brown. It's certainly does reduce though.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 03-15-2019, 07:03 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,698
Jordan Kube is on a distinguished road
Just remember, Josh, you are made of stardust. Practically a living god. You need not concern yourself with such terrestrial things as the smell of sulphur.

Or: To quote Ed Skeels, "It's ok to have a pussy, it's not ok to be one."

Or: To quote Father Guido Sarducci "You won't be sorry for long."

Totally kidding but I tend to just go for stuff like this. Melt it as is.
__________________
WWUD? Think for yourself.

Last edited by Jordan Kube; 03-15-2019 at 10:13 PM.
Reply With Quote
  #6  
Old 03-15-2019, 07:41 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,506
Pete VanderLaan is on a distinguished road
"You can almost always get it out of the pot"

Pete V
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 03-16-2019, 06:25 PM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 650
Josh Bernbaum is on a distinguished road
Thats pretty funny Jordan. I've heard through the grapevine that Lino likes Gaffer's durissimo better than the rosin he used to use. That may or may not be true but I think it's true. Quenching this durissimo doesn't turn the water black or anything like that, not sure if that's an indication of whether or not there's rosin in there.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #8  
Old 03-17-2019, 02:37 AM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,698
Jordan Kube is on a distinguished road
I believe it. It's a great glass but if you add in the duro stiffness it's probably even better. I wonder if John saw this formula and tweaked it. He wasn't working on anything like this when I talked to him in Corning at the GAS conference. Another note, this isn't a casing glass. Blows out garbage just like the duro. Only for cane work, threading, lip wraps etc. Melt it and make it into bar.
__________________
WWUD? Think for yourself.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:42 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.