Quote:
Originally Posted by Marc Carmen View Post
Josh, I'm dying to try the durissimo. If it's a similar formula to Nero duro then it's a lead free iron sulfide black. Iron sulfide glass is not only naturally stiff but also incredibly brittle. Old glass container literature mentions that it is a cheap and easy way to black glass, if only it didn't make such an impractically brittle bottle.

Man, I have sooo many bubbly black filigrana in my student work haha.
It's not just stiff, it's CRAZY stiff! Definitely the stiffest glass I've ever played with and makes the white duro feel like enamel. I gather on the new black the instant it stops moving, which is literally walking from the gh to the furnace. If you lose the core heat you're toast. If you don't transfer it directly to a stick you're toast. Gathers needs to be done before the previous one fully sets up. Pulls need to be really hot with a faster walk than usual. If you don't have the black poking out of the end of the setup and quench before you stick to the post, you're toast. It's actually super fun to work with because it's so quirky. I've not had great luck keeping it jet black--I think it might have something to do with our gh running a bit rich (maybe Pete can explain what's up w/this). It's been going graphite grey on me--I'm going a few things to try to avoid this. I've been pulling it into cane, then bundling the cane and making murrine. I haven't used the murrine yet, but it looks excellent.

If you're into twisty cane, definitely try some of this stuff, it's wild and so much fun.

Last edited by David Patchen; 11-03-2017 at 12:17 AM.
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:08 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.