Question Watlow programming question

I am rewriting some programs on my furnace controller. There is an option " wait for process crossover value (WPr)" that applies to soak steps. Reading the manual it seems that this says wait until the previous step value / temp is reached before starting the soak. So if I am reading this correctly if step 1 is get to 500 degrees in two hours and then step 2 is soak for an hour Wif Pr set to true will only start the soak step after it reaches 500. If step 1 is 450 after 2 hours the soak timer won't start but once the furnace reaches 500, even if that is 5 hours later then the soak step will start. Is this correct? Many thanks.
Art
Reply With Quote
  #2  
Old 06-13-2020, 08:59 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,850
Eben Horton is on a distinguished road
Sounds right.
__________________
<EBEN EΠOIESEN >
Reply With Quote
  #3  
Old 06-13-2020, 09:27 PM
Patrick Casanova Patrick Casanova is offline
Registered User
 
Join Date: Apr 2002
Location: Western Wisconsin
Posts: 289
Patrick Casanova is on a distinguished road
I ran an Watlow 8CLS for 20 years... Yes Some times it can be more problematic coming down if your annealer cools slower than the time set for the segment. The next segment won't start until you reach the set point called for in that segment, even though the time set had.
Reply With Quote
  #4  
Old 06-14-2020, 07:37 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,850
Eben Horton is on a distinguished road
Quote:
Originally Posted by Patrick Casanova View Post
I ran an Watlow 8CLS for 20 years... Yes Some times it can be more problematic coming down if your annealer cools slower than the time set for the segment. The next segment won't start until you reach the set point called for in that segment, even though the time set had.
Thatís why I have a fiber blanket walled annealer. It drops at just the right rate and I can control cooldowns 100%.
__________________
<EBEN EΠOIESEN >
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 06:22 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.