Type S Thermocouple

It is time to start going through all the extra backup parts that I've accumulated over the years. I have two Type S thermocouples for sale. Both were back to Pyromation for testing and calibration this spring. They are in like new condition. One has a "corrosive environment" protective sleeve attached to the head. The other has a mullite shield that I used as is in ovens, or slid it into the protective tube in my furnace crown. When bringing a new furnace up to temp I placed two additional probes in various spots to monitor the evenness of the temperature within the chamber. I also used them in my ovens to test the same thing as well. Feel free to ask any questions. Both are 12" long. $300 for either one.

Images to come...
Reply With Quote
  #2  
Old 06-15-2017, 03:15 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,089
Pete VanderLaan is on a distinguished road
That's a very nice price for those Pat. I have a number of both Type S and R which I have had in service since 1976 and they are all fine. Just replace the mullite protection tube on a regular basis and they simply will last forever.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 07-30-2017, 12:54 PM
Daniel Sviland Daniel Sviland is offline
Registered User
 
Join Date: Apr 2012
Location: Waukegan, IL
Posts: 15
Daniel Sviland is on a distinguished road
Mullite Tube

Does anyone know the size of the Mullite tubes used in a Stadelman 300#- getting ready for a rebuild and apparently this one has never been changed in 11 years. Feeling lucky!

Would rather get it in stock before I turn down
Thanks,
Dan
Reply With Quote
  #4  
Old 07-30-2017, 02:19 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 861
Sky Campbell is on a distinguished road
Quote:
Originally Posted by Daniel Sviland View Post
Would rather get it in stock before I turn down
Thanks,
Dan
And unstuck before turn down. That is if you want to remove it in one piece.

You can always unscrew the weather head pull the tc wire and use a unisulated wire to measure length. The diameter should be easy to measure from the outside. I've found it's cheap enough to replace the whole weather head then trying to mortar a new protection tube into a old weather head.
Reply With Quote
  #5  
Old 07-30-2017, 06:18 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,089
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Daniel Sviland View Post
Does anyone know the size of the Mullite tubes used in a Stadelman 300#- getting ready for a rebuild and apparently this one has never been changed in 11 years. Feeling lucky!

Would rather get it in stock before I turn down
Thanks,
Dan
******
Your tube came from Grant / Edgell which is in either Seattle or Portland.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 07-31-2017, 11:14 AM
Patrick Casanova Patrick Casanova is offline
Registered User
 
Join Date: Apr 2002
Location: Western Wisconsin
Posts: 268
Patrick Casanova is on a distinguished road
Thank you!
Both are sold.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:43 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.