Blow and cap

I never got the blow and cap method to work for me. My blow hose works well . What’s the secrete of the blow and cap?
Franklin
Reply With Quote
  #2  
Old 10-11-2019, 10:19 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 460
Shawn Everette is on a distinguished road
Practice. You want a good amount of pressure in the pipe and your thumb ready to go. Try it on a cold plugged pipe, if you hear air move when you take your thumb away you did it right.
Reply With Quote
  #3  
Old 10-11-2019, 11:34 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,573
Pete VanderLaan is on a distinguished road
I would think that doing that with a hose was going to really require a good deal more pressure than just doing it with a blowpipe. Is that bad thinking?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 10-11-2019, 11:43 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 460
Shawn Everette is on a distinguished road
You cant exactly do it with the hose. Blow, cap, bubble, then hose.
Reply With Quote
  #5  
Old 10-11-2019, 02:10 PM
Rich Simmons's Avatar
Rich Simmons Rich Simmons is offline
Registered User
 
Join Date: Aug 2018
Location: California
Posts: 38
Rich Simmons is on a distinguished road
Try this Video -
https://www.glassblowersguide.com/bl...pping-a-bubble

I've never met Nikolaj Christensen, but I like his explanation.
Reply With Quote
  #6  
Old 10-11-2019, 02:34 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 460
Shawn Everette is on a distinguished road
Ugg, fat derlin mouthpieces.
Reply With Quote
  #7  
Old 10-11-2019, 11:43 AM
Warren Trefz Warren Trefz is offline
Registered User
 
Join Date: Oct 2003
Location: Batavia, OH
Posts: 66
Warren Trefz is on a distinguished road
Have the bottom part of you thumb pad resting on the mouthpiece almost covering the opening completely, so that you can easily seal it off, and then place the mouthpiece and positioned thumb in your mouth from the side. Blow and seal off the pipe while you are blowing. Should look sort of like you are playing a flute but with a thumb in you mouth also. As Shawn said practice on a clogged pipe by getting it hot and try capping. Hold it up to your ear and uncap it and if you hear a pop you had it sealed. When you start capping with molten glass it does not take a lot of pressure, the heat will do the work for you. If you are blowing bottle glass, which if I remember you are, it will take a bit more pressure for the capping puff. But heat does wonders.
Reply With Quote
  #8  
Old 10-11-2019, 03:54 PM
David Russell David Russell is offline
Registered User
 
Join Date: Jul 2008
Location: South Carolina
Posts: 216
David Russell is on a distinguished road
When I learned I found it helpful to excessively overdue the amount of air being blown before capping.

Last edited by David Russell; 10-11-2019 at 04:30 PM.
Reply With Quote
  #9  
Old 10-11-2019, 09:43 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,953
Franklin Sankar is on a distinguished road
Great video. He can teach well.
Thanks
Franklin
Reply With Quote
  #10  
Old 10-12-2019, 07:35 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,591
Eben Horton is on a distinguished road
Practice on a clogged pipe. Release the air near your ear to know if you got it right. The more you practice the easier it gets.
__________________
<eben epoiese>
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 01:09 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.