Sourcing 0/3/4 pumice?

I used to just go down to the pumice plant and buy it by the bag when I lived in Santa Fe. That option is gone, the plant moved etc. I find I still need that grade pumice and wonder if anyone has a source that is actually selling it. It's the same grit that dentists use but they have this perfumed crap.
So, Active suppliers?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #2  
Old 10-17-2019, 12:59 PM
Rick Kellner Rick Kellner is offline
Registered User
 
Join Date: Jan 2004
Location: Hillsboro, OR
Posts: 196
Rick Kellner is on a distinguished road
You can buy it unscented for the laboratory side of the dental field, but some of the supply houses will not sell to entities outside of the profession. Others might require only a business license. If you look hard enough, there are some without such hassles, but they are usually peddling on eBay, etc.

Here's an example of the lab stuff:

https://www.pearsonlab.com/catalog/p...3906&pid=50609
Reply With Quote
  #3  
Old 10-17-2019, 02:22 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,583
Pete VanderLaan is on a distinguished road
I found a place that will sell it to me at a very nice price 90Lbs for $37.00 BUT they won't ship to a residential address, something I've hit before buying Nitric acid.
Fed Ex has seized on this residential address listing which was done by some arbitrary means and it is killing shipping crucibles right now. Many studios are not in business districts even to the point of not being allowed in business districts so it's a catch 22.
With the pumice, all I've been able to do is to explain that pumice isn't exactly a chemical, it's a mineral. We'll see. A dental supply refused to sell it to me.

Used to be I'd drive down St Francis Drive in Santa Fe and get it at the Navaho plant. The city grew up around the facility and the neighbors who had all bought the vacant lots around the place started to complain to the city. The facility was grandfathered in but eventually the pressure turned into a nuisance and they left town. Now, I'm 2500 miles away looking for a crummy bag of 0 3/4 pumice. The 90 lb bag used to cost me nine bucks. I gave them cash to use at Dunkin Doughnuts.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 10-17-2019, 02:30 PM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,595
Eben Horton is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
I found a place that will sell it to me at a very nice price 90Lbs for $37.00 BUT they won't ship to a residential address, something I've hit before buying Nitric acid.
Fed Ex has seized on this residential address listing which was done by some arbitrary means and it is killing shipping crucibles right now. Many studios are not in business districts even to the point of not being allowed in business districts so it's a catch 22.
With the pumice, all I've been able to do is to explain that pumice isn't exactly a chemical, it's a mineral. We'll see. A dental supply refused to sell it to me.

Used to be I'd drive down St Francis Drive in Santa Fe and get it at the Navaho plant. The city grew up around the facility and the neighbors who had all bought the vacant lots around the place started to complain to the city. The facility was grandfathered in but eventually the pressure turned into a nuisance and they left town. Now, I'm 2500 miles away looking for a crummy bag of 0 3/4 pumice. The 90 lb bag used to cost me nine bucks. I gave them cash to use at Dunkin Doughnuts.
Does Karissa still have her gallery? Ship it to her.
__________________
<eben epoiese>
Reply With Quote
  #5  
Old 10-17-2019, 06:59 PM
Steven O'Day Steven O'Day is offline
Registered User
 
Join Date: Jun 2002
Location: portland oregon
Posts: 319
Steven O'Day is on a distinguished road
I picked up bags that fell off the truck when I lived there!
Reply With Quote
  #6  
Old 10-17-2019, 07:58 PM
Kenny Pieper Kenny Pieper is offline
Registered User
 
Join Date: Feb 2003
Location: Burnsville N.C.
Posts: 836
Kenny Pieper is on a distinguished road
I think I got my Navajo pumice from cr minerals last time. I got a 50lb bag and it was big and cheap.
Reply With Quote
  #7  
Old 10-18-2019, 03:10 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,583
Pete VanderLaan is on a distinguished road
That's funny. CR Minerals bought out American Pumice which had the plant in Santa Fe I used to get it from. They moved to Pueblo Colorado, home of polluting industries everywhere. The website shot is of the Sangre De Cristo Mountains, behind Santa Fe. The Jemez Mountains are just chock full of this stuff. It used to have the downside of a high iron content. We would put magnets in the slurry tray and at the end of the day, it looked like a miniature porcupine.

Thanks for the name link Kenny.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 10-28-2019, 03:17 PM
Hugh Jenkins Hugh Jenkins is offline
Registered User
 
Join Date: Sep 2006
Location: Honoka'a, HI
Posts: 990
Hugh Jenkins is on a distinguished road
I am using a product called Resilience that is a dental compound. I once got a 5kg box as a "sample". I still like using it between 20 micron alumina and cerium but don't do near as much polishing as I once did.

Since I have finally decided to keep going until at least when I run out of glass or the crucible signs off, I am cleaning up my cold work area for whatever comes, so there will certainly be a need for touch ups if nothing else.
__________________
Aloha, Hugh
Reply With Quote
  #9  
Old 10-28-2019, 04:21 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,583
Pete VanderLaan is on a distinguished road
I remeber Nick Labino putting blanks away. it never really worked out sadly. I am refurbishing all the heads on the pumice and cerium, the diamond saw is getting cleaned. Since I went to not having a helper, my 120 machine has stayed true for 14 remarkable years. I do think I'll need to check bearings and it's really hard for me to pull a 300 lb wheelhead alone. The furnace got quite small last year and when the futures propane runs out, I'll really change this dog and pony show.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #10  
Old 10-28-2019, 08:45 PM
Hugh Jenkins Hugh Jenkins is offline
Registered User
 
Join Date: Sep 2006
Location: Honoka'a, HI
Posts: 990
Hugh Jenkins is on a distinguished road
Getting rid of the pony makes a big difference.
__________________
Aloha, Hugh
Reply With Quote
  #11  
Old 10-29-2019, 08:52 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,583
Pete VanderLaan is on a distinguished road
and they aren't even metaphorical. We have three hay burners.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #12  
Old 11-02-2019, 07:23 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 766
Michael Ahlefeldt-Laurvig is on a distinguished road
Since I went to not having a helper, my 120 machine has stayed true for 14 remarkable years.

Thats really funny!
Reply With Quote
  #13  
Old 11-02-2019, 08:13 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,583
Pete VanderLaan is on a distinguished road
furthermore, all my tools are right where I left them the day before.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #14  
Old 11-17-2019, 05:40 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,583
Pete VanderLaan is on a distinguished road
Ultimately , I got a 45 lb bag from these guys, being the only ones willing to answer an email. The price was OK at about $25.00. The shipping was twice that.

https://pumicestore.com/pumice-grades-directory.html
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 02:08 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.