Question for cullet users

So, recently, I got email from a glassperson who indicated that the hood in the shop he works out of has been crudding up with all too familiar fluff. My regular experience with the phenomenon was a borax residue and those are always yellowish, notably forming around the door at either a one o'clock or and eleven o'clock position, but he indicated that it was white. That takes me elsewhere.

So, What I would like to know is whether anyone else is experiencing this stuff. I have a strong suspicion as to what it is and where it might come from but first, I'd like to hear from the legions. I don't view it as insignificant.

White, not yellow.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #2  
Old 11-28-2019, 07:06 PM
Art Freas Art Freas is online now
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 587
Art Freas is on a distinguished road
We had some of it with the no borax Spectrum System 96 improved studio nuggets. There was less of if than the borax fluff but it was noticable.
Reply With Quote
  #3  
Old 11-29-2019, 01:12 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,572
Pete VanderLaan is on a distinguished road
What cullet do you use now? Does it show any residue or something like that on the cullet?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 12-02-2019, 12:51 PM
Shawn Everette Shawn Everette is online now
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 460
Shawn Everette is on a distinguished road
When I was using cristalica my fluff was white, not yellow. Made massive cakes on a girder above the flue. Assumed it was the borax.
Reply With Quote
  #5  
Old 12-04-2019, 04:52 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,702
Jordan Kube is on a distinguished road
I've always encountered white stuff. Toss it in some water and the water gets "slippery". Sodium and/or Boron.
__________________
WWUD? Think for yourself.
Reply With Quote
  #6  
Old 12-09-2019, 03:26 PM
Art Freas Art Freas is online now
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 587
Art Freas is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
What cullet do you use now? Does it show any residue or something like that on the cullet?
Cristallica, mostly white fluff now, a bit of yellow not bright like S96 Studio
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 11:34 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.