Old 04-10-2019, 09:28 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,953
Franklin Sankar is on a distinguished road
Why that working temperature

I started to reduce the furnace temperature gradually over the last year because felt that if the melted glass was still viscous at the lower temperatures that was ok. Then I forgot I reduced the temperature and started to get all kinds of problems.
So the question is how did you choose the working temperature for your furnace.
I noticed some people would have one temp and others another.

Franklin
Reply With Quote
  #2  
Old 04-11-2019, 08:16 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,573
Pete VanderLaan is on a distinguished road
you tool up for what you are making.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 04-11-2019, 09:38 AM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,591
Eben Horton is on a distinguished road
The hotter the glass the smaller your gathers. The colder the glass the bigger the gathers can be but it comes at a cost of working time and the possibility of bubbles forming from your gather tails folding over them selves.

I usually keep my furnace at 1970 when I am working. The defecto working temp at most schools and public access studios is 2100 which I think is too hot for production.
__________________
<eben epoiese>
Reply With Quote
  #4  
Old 04-11-2019, 10:11 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 460
Shawn Everette is on a distinguished road
I agree with Eben, it's more a matter of preference. I keep mine about 2100 in general, but I actually like doing my production session after a fresh charge while it's still piping hot. I like sloppy bits that need no reheat.

What you are actually batching is going to have a pretty drastic change on ideal fining and working temp.

You can gauge temp with either a controller or pyrometer, or go old school and tell by color. You'll get the eye for color eventually either way.
Reply With Quote
  #5  
Old 04-11-2019, 08:10 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 588
Art Freas is on a distinguished road
We are working with the Cristalica and initially we tried 2100 but it was just too thick to get the gathers we wanted. It was hard to get the right amount to work thin without taking a lot off the pipe. We now work at 2125.
Reply With Quote
  #6  
Old 04-11-2019, 09:08 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,953
Franklin Sankar is on a distinguished road
My Wire elements won’t like 2100. It is interesting that 25 deg. makes such a difference in gathering.
Franklin
Reply With Quote
  #7  
Old 04-12-2019, 08:51 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,573
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Art Freas View Post
We are working with the Cristalica and initially we tried 2100 but it was just too thick to get the gathers we wanted. It was hard to get the right amount to work thin without taking a lot off the pipe. We now work at 2125.
****
That's what I meant when I said you tool up for what you are making. Efficiency keeps you from being exhausted. Sometimes you can turn it down, sometimes up. That's far more flexible than most tooling in the shop.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 12:10 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.