you can make your own silver chloride using the directions in Glassnotes 3. Henry hated the way I made silver Nitrate and thought I was a menace to society. I haven't changed. It looks like a mad science experiment when I do it but I hate waiting around. You can also make iodide and bromide from glassnotes as well. With iodide, you can draw on the glass. The sodium bromide and sodium Iodide are what will cost you since they come as a reagent grade. I think Noah handles both.

I always had trouble with Simpson trying to do too many things all at once. He consistently would add all sorts of shit to the Corona formula and frequently made it quite incompatible and rick expected me to fix it. . It was tiring.
No it won't flow between gathers.
Using too much is not a good thing for a variety of reasons.
Learn your basics well first. The silver has not brought you to your knees yet, but it will.
Good Design is way harder than any of this stuff.
__________________
Where are we going and why am I in this basket?
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 08:36 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.