Purple Aventurine

I was reading about aventurine in Wikepedia and it mentioned that there was a purple aventurine. Has anyone seen this running around or used it?
Reply With Quote
  #2  
Old 08-14-2018, 10:42 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,765
Eben Horton is on a distinguished road
Iíve seen blue and worked with it , but I donít see why purple couldnít exist.. I have never seen it though.
__________________
<eben epoiese>
Reply With Quote
  #3  
Old 08-14-2018, 11:41 AM
Eric Trulson Eric Trulson is offline
Young Turk
 
Join Date: Sep 2014
Location: Stanwood, WA
Posts: 143
Eric Trulson is on a distinguished road
I have a vague memory of coming across some big chunks of purple and gold/brown aventurine in a dusty old cardboard box under the color shelves at Snow Farm last summer. (Which is totally unhelpful as far as an original source, but at least confirms it exists.)

To tack on to Art's original question, does anybody know of glass folks who are melting/have melted their own aventurine?

Gaffer makes a nice lime green one, and I know Lino and one or two other old-schoolers from Murano will occasionally use it in their work (not sure if they melt it in-house or get it from someone else on the island). I've never heard of it being melted elsewhere though.
Reply With Quote
  #4  
Old 08-14-2018, 11:54 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,120
Pete VanderLaan is on a distinguished road
There are two traditional aventurines out there and both are produced by cooling the pot of glass and taking out the chunks. Those are chrome and copper respectively. It would be the case I'd imagine that cobalt could be added to either of those glasses.
It's not to be confused with the glasses where a bunch of mica is getting thrown in. Sparkly but not the same. given their positions on the atomic table, I have to wonder aloud if an aventurine could theoretically be made with either silver or gold. Either would really be pretty expensive if it could work at all.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 08-14-2018, 12:00 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,120
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Art Freas View Post
I was reading about aventurine in Wikepedia and it mentioned that there was a purple aventurine. Has anyone seen this running around or used it?
**********
I went to wikipedia and keyed in aventurine and can't find a reference that you might be referring to. Perhaps you could put up the direct link?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 08-14-2018, 12:32 PM
Rich Simmons's Avatar
Rich Simmons Rich Simmons is offline
Activist
 
Join Date: Aug 2018
Location: California
Posts: 39
Rich Simmons is on a distinguished road
I've played with it, and still have some big chunks. I tried to pickup a piece about the size of a peach pit straight on the pipe and blow it out with two gathers over it. Didn't work out so well, it's incompatible (at least this process was with a large chunk) I'll post a pic of the vase tonight when I get home.

Last edited by Rich Simmons; 08-14-2018 at 01:20 PM.
Reply With Quote
  #7  
Old 08-14-2018, 01:07 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,765
Eben Horton is on a distinguished road
Quote:
Originally Posted by Rich Simmons View Post
I've played with it, and still have some big chunks. I tried to pickup and piece about the size of a peach pit straight on the pipe and blow it out with two gathers over it. Didn't work out so well, it's incompatible (at least this process was with a large chunk) I'll post a pic of the vase tonight when I get home.
I wil take that incompatable glass off of your hands
__________________
<eben epoiese>
Reply With Quote
  #8  
Old 08-14-2018, 01:30 PM
Rich Simmons's Avatar
Rich Simmons Rich Simmons is offline
Activist
 
Join Date: Aug 2018
Location: California
Posts: 39
Rich Simmons is on a distinguished road
I'll post some pic's first. Compared to other aventurine I've used it doesn't have quite the same bling.

Last edited by Rich Simmons; 08-14-2018 at 01:59 PM.
Reply With Quote
  #9  
Old 08-14-2018, 03:05 PM
Rich Simmons's Avatar
Rich Simmons Rich Simmons is offline
Activist
 
Join Date: Aug 2018
Location: California
Posts: 39
Rich Simmons is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
**********
I went to wikipedia and keyed in aventurine and can't find a reference that you might be referring to. Perhaps you could put up the direct link?
I think he ended up looking at the goldstone wiki - It does mention blue and purple variations.
Reply With Quote
  #10  
Old 08-14-2018, 05:12 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,120
Pete VanderLaan is on a distinguished road
"goldstone is more marketing, less science and glass historical chemistry."

You gonna believe what you need to believe.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #11  
Old 08-14-2018, 05:16 PM
Rich Simmons's Avatar
Rich Simmons Rich Simmons is offline
Activist
 
Join Date: Aug 2018
Location: California
Posts: 39
Rich Simmons is on a distinguished road
Just Sayn' - Not making any claims about Wiki's accuracy on any subject..
Reply With Quote
  #12  
Old 08-14-2018, 05:29 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,120
Pete VanderLaan is on a distinguished road
Really? What a shock!
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #13  
Old 08-14-2018, 05:33 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Registered User
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,231
Greg Vriethoff is on a distinguished road
Yes, Wikipedia is a source that should be approached with caution.

That being said, here you go:

"Cobalt or manganese can be substituted for copper; the resulting crystals have a more silvery appearance and are suspended in a strongly colored matrix of the corresponding ionic color, resulting in blue goldstone or purple goldstone respectively."

Tumble_Polished_Blue_Goldstone_.jpg

I guess the pic shows blue. Maybe you could argue "violet"?
__________________
Temperature and time.
Reply With Quote
  #14  
Old 08-14-2018, 05:40 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Registered User
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,231
Greg Vriethoff is on a distinguished road
It's worth noting that this blurb about cobalt and manganese does not site a direct source.

I have not reviewed either of the stated sources that the article sites.

Also worth noting is how little is referenced at all.

If anyone wants to go down this rabbit hole please report back with any discoveries gathered in the field. Your input is always appreciated.
__________________
Temperature and time.
Reply With Quote
  #15  
Old 08-14-2018, 05:59 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,120
Pete VanderLaan is on a distinguished road
I would want to hear from John. Otherwise. it's just junk.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #16  
Old 08-14-2018, 07:49 PM
Art Freas Art Freas is online now
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 694
Art Freas is on a distinguished road
Quote:
Originally Posted by Greg Vriethoff View Post

This is the sentence that sent me down the rabbit hole.
Reply With Quote
  #17  
Old 08-14-2018, 07:51 PM
Terry Crider
Guest
 
Posts: n/a
I googled Purple Aventurine and it came up as rock/stone---
Lapidary stuff
Reply With Quote
  #18  
Old 08-14-2018, 08:19 PM
Rich Simmons's Avatar
Rich Simmons Rich Simmons is offline
Activist
 
Join Date: Aug 2018
Location: California
Posts: 39
Rich Simmons is on a distinguished road
Here's a pic of the test vase I made as mentioned above. Broken up the stuff works fine but it's not got any wow factor. Oh, and Pete - I was just pointing out where the purple reference came from, no need to be a Dick about it!
Attached Images
File Type: jpg IMG_0367.jpg (49.0 KB, 74 views)
Reply With Quote
  #19  
Old 08-14-2018, 08:22 PM
Marty Kremer Marty Kremer is offline
Registered User
 
Join Date: May 2004
Location: North Yarmouth ME
Posts: 517
Marty Kremer is on a distinguished road
This won't help you blowers but Bullseye's got a cobalt aventurine (that I pushed them to make) in stock. It's come out turquoise-y sometimes but is usually a rich dark cobalt. Fun to play with, for fusers anyway.
Reply With Quote
  #20  
Old 08-15-2018, 12:12 AM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,551
Rich Samuel is on a distinguished road
No real chemistry here, but an interesting history.

https://abfabtreasures.wordpress.com...nd-aventurine/
Reply With Quote
  #21  
Old 08-15-2018, 07:59 AM
Kenny Pieper Kenny Pieper is offline
Registered User
 
Join Date: Feb 2003
Location: Burnsville N.C.
Posts: 844
Kenny Pieper is on a distinguished road
We have a mineral and gem festive here in Spruce Pine once a year in august that has venders from all over the U.S.. There is usually a guy there that has a 55 gallon steel drum of the gold aventurine. He sales it for $10lb.
I use to use it a lot in cane goblets. It tricky to work with in that the copper if heated too much will go back into solution especially on the surface. I found that I need to heat it as little as possible before gathering and it doesn't blow out all that well. If it gets thin is looses its effect.
Attached Images
File Type: jpg gold and goldstone cane goblets detail.jpg (18.9 KB, 50 views)
Reply With Quote
  #22  
Old 08-15-2018, 08:25 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,120
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Rich Simmons View Post
Oh, and Pete - I was just pointing out where the purple reference came from, no need to be a Dick about it!
**********
You think I was being a Dick about it? Which comment? This one?

********
(To Art, directly)"I went to wikipedia and keyed in aventurine and can't find a reference that you might be referring to. Perhaps you could put up the direct link?"
********
Or this? (regarding the veracity of Wikipedia)
**********
"Really, what a shock!"
**********
"I would want to hear from John. Otherwise. it's just junk."
**********
So, you haven't really gotten a dose of when I do want to be a dick about something with five posts under your belt. I do spend a lot of my time here correcting misconceptions about glass. I think I spent about two years trying to get people to stop calling it "Adventurine"
The Mica add ons are not aventurines in any true sense and my great adherence is to understanding colored glass and the how and why's of what it does.
Cobalt is an interesting material in that it is a true saturation colorant. It doesn't set up suspensions, or colloidal strands, or crystals. It's more like India Ink on a white carpet. Try getting it out of the carpet. So, cobalt can be used to tint other colors without changing their internal prime directives. Cobalt on top of silver glasses can make blues, greens and occasional streaky purples. Cobalt can taint a copper aventurine from a sparkly gold color into a purple I suppose but it will be really dark and very tough to balance based on thickness as the color will change based on transmissivity. The other references, near as I can see are what Terry Crider saw- lapidary materials and they aren't glasses. I do like rocks though.

I think it's far more fruitful to think about what color the casing gather should be over a true aventurine if you want to present a different color.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #23  
Old 08-15-2018, 10:53 AM
Rich Simmons's Avatar
Rich Simmons Rich Simmons is offline
Activist
 
Join Date: Aug 2018
Location: California
Posts: 39
Rich Simmons is on a distinguished road
These comments don't contribute anything to the topic and IMO didn't do anything to help Art:

Or this? (regarding the veracity of Wikileaks) Uh, Wikipedia. Wikileaks is a totally different site buddy.
**********
"Really, what a shock!" Trying to point to the reference, I don't need a litany of posts to see your response to this wasn't helpful.
**********
"I would want to hear from John. Otherwise. it's just junk." Yeah, really helpful.

You're a moderator, Right? You end the last thread with helpful information.

Last edited by Rich Simmons; 08-15-2018 at 10:55 AM.
Reply With Quote
  #24  
Old 08-15-2018, 12:23 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is online now
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 1,080
Mark Rosenbaum is on a distinguished road
Wow, 6 posts and you are slamming the moderator!
You need to start to understand Pete's responses. 23 responses and the topic hasn't completely gone off the rails, that is unusual. Tangents and rabbit holes are very common here.
Reply With Quote
  #25  
Old 08-15-2018, 12:32 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,120
Pete VanderLaan is on a distinguished road
well, wiki leaks is probably more on my mind than wikipedia so I would apologize for that misdirective. When it comes to glass, Wikipedia is one of the last places I would be inclined to search. I have been to read all about goldstone and it sounds rather fishy to me particularly when it's shown as a finished product in a slick fashion. On the other hand, if I google "Aventurine Glass" I can get to Murano work which is all either chrome green or copper colors as additives to other pieces but nothing I see that says purple or anything to that effect. That is consistent with what I know and the initial question was about purple aventurine.

As to John, John Croucher is who I refer to and is far more versed in the chemistry of glass than I am. If John tells me that Goldstone is actual aventurine, including a purple one, I'll believe it. Otherwise I'll stick to my opening statement asking for a referral on Aventurine, not goldstone. At one point in Wikipedia, it's referred to "as a form of quartz " and that certainly is inaccurate at its best.

I'm not big on misinformation here, subsequently, finding verifiable source is what I look for. Wikipedia certainly didn't cut it as yet another poster tried to point out as being quite likely. But it does sound official.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 09:40 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.