Charley's gas saver

Any update on the revised product, Charles? I'm not seeing anything in the National Torch website, or elsewhere on the web, so now I'm curious.
Reply With Quote
  #2  
Old 08-02-2019, 11:54 AM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 621
Charles Friedman is on a distinguished road
Charley's Gas Saver was introduced at the GAS 2019 St. Pete Conference and then at the Scientific Glass Blowing Conference at Corning 2019. Web sites and ads are being updated now. Here was the Flyer handed out from both National and Wale. Need to call them. There is a new CGS "Bench Model" coming.
Attached Images
File Type: jpg Wale CGS ad back.jpg (51.9 KB, 75 views)
File Type: jpg Wale CGS ad front.jpg (60.7 KB, 61 views)
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
  #3  
Old 08-28-2019, 12:26 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 621
Charles Friedman is on a distinguished road
Here is National's web page.
https://nationaltorch.com/charleys-gas-saver/

Wales page will coming on line in Sept.
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
  #4  
Old 08-28-2019, 02:17 PM
Rick Kellner Rick Kellner is offline
Registered User
 
Join Date: Jan 2004
Location: Hillsboro, OR
Posts: 203
Rick Kellner is on a distinguished road
Thank you. I had been looking again on their site recently, but it must have been newly added. Was getting worried that I might have to invest in an old skool gas saver instead!
Reply With Quote
  #5  
Old 08-28-2019, 02:53 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 771
Art Freas is on a distinguished road
Is this self lighting when you close the handle?
Reply With Quote
  #6  
Old 08-28-2019, 02:58 PM
Rick Kellner Rick Kellner is offline
Registered User
 
Join Date: Jan 2004
Location: Hillsboro, OR
Posts: 203
Rick Kellner is on a distinguished road
Pretty sure it's like the first iteration, in that you need to furnish a separate pilot device, like an electronic sparker, bunsen burner, etc.
Reply With Quote
  #7  
Old 08-28-2019, 05:29 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 621
Charles Friedman is on a distinguished road
Here are some on-demand pilot lights. It will not let me post my info about "Fireboy" and 4 way electronic ignitors. I have CGS if you are in need.
__________________
"Glass will save the world from ourselfs" CharlesF

Last edited by Charles Friedman; 08-28-2019 at 05:41 PM.
Reply With Quote
  #8  
Old 08-29-2019, 11:01 AM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 771
Art Freas is on a distinguished road
Quote:
Originally Posted by Charles Friedman View Post
Here are some on-demand pilot lights. It will not let me post my info about "Fireboy" and 4 way electronic ignitors. I have CGS if you are in need.
Not seeing a link in this post.
Reply With Quote
  #9  
Old 08-29-2019, 12:36 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 621
Charles Friedman is on a distinguished road
Pilot lights

try these.


https://www.ebay.com/sch/i.html?_nkw...nsen+Burner%2C



https://jetsinc.com/tools-and-suppli...d-touch-spark/
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
  #10  
Old 08-31-2019, 02:42 PM
Scott Dunahee's Avatar
Scott Dunahee Scott Dunahee is offline
Registered User
 
Join Date: Apr 2002
Location: Madison, WI
Posts: 646
Scott Dunahee is on a distinguished road
I had one of those touch igniters (Charles' last link) on my torch cart in my shop. I was pleasantly surprised at the durability of it and I never changed the batteries once, which shocked me. 3 years of service use?

Anyway, good stuff. Intuitive to use after trying it once.

BSD
__________________
That's all right. I never expected there to be a blue light special on enlightenment...
Reply With Quote
  #11  
Old 09-01-2019, 02:26 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 621
Charles Friedman is on a distinguished road
The thing to remember about using a battery ignitor is: ACTIVATE THE SPARKER FIRST, before you squeeze the handle and call for gases. If you do the reverse, you will be sending a ball of gas toward the sparker and when activated it will make a ball of fire. Not good. Since it is a open system (not closed up) the unit will just blow out the battery cover first, it will not blow up like a hand grenade.
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 03:24 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.