Instant Batch Room

I though about building walls for a batch room and then remembered how cheap an 8' x 8' grow tent is these days. Nice thick walls, holes for vacuum or ventilation. I've got a Grizzley 2 stage HEPA cyclone dust extractor but I still have to figure out how to get the make up air just right. It sucks the walls of the tent in pretty good. It's actually working really well without it. Bulk chemicals on a pallet on the left, stainless table with shelving for colorants on the right. Mixer and floor scale along the back. I also have a dehumidifier that keeps the RH right at 35%.

This is really all the room you need to do it yourself. I've got space on the pallet for about 2000 pounds of bulk chemicals and the stainless table is perfect for everything else. I still have room for a trash can and small shop vac with HEPA filter. Best part is, I can roll it up and throw it in the garbage when I'm done.
Attached Images
File Type: jpg Batch room resize.jpg (49.9 KB, 74 views)
__________________
WWUD? Think for yourself.
Reply With Quote
  #2  
Old 01-10-2018, 10:31 PM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,875
Eben Horton is on a distinguished road
“Let’s cook....”

That’s awesome Jordan!
Reply With Quote
  #3  
Old 01-11-2018, 12:55 AM
David Patchen's Avatar
David Patchen David Patchen is online now
Registered User
 
Join Date: Sep 2005
Location: San Francisco, CA
Posts: 1,919
David Patchen is on a distinguished road
Quote:
Originally Posted by Jordan Kube View Post
Best part is, I can roll it up and throw it in the garbage when I'm done.
New category for recycling: Inflatable Batch Room
Reply With Quote
  #4  
Old 01-11-2018, 10:15 AM
Scott Novota's Avatar
Scott Novota Scott Novota is offline
AbbyNormal User
 
Join Date: Jan 2004
Location: Pensacola Florida
Posts: 2,180
Scott Novota is on a distinguished road
Ok I am totally doing this. We are rebuilding the layout in the shop currently and I can work this right into a dead corner.

Thanks for posting what a great idea.

Is that the:

Matrix Horticulture 96"x96"x80"

Last edited by Scott Novota; 01-11-2018 at 10:16 AM. Reason: added content.
Reply With Quote
  #5  
Old 01-11-2018, 11:05 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,790
Pete VanderLaan is on a distinguished road
I'm way too much of a slob to ever do it this way. I also have way too many bags and buckets of stuff you can't get anymore. It sure looks like it would do well.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 01-11-2018, 11:42 AM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,750
Jordan Kube is on a distinguished road
Quote:
Originally Posted by Scott Novota View Post
Ok I am totally doing this. We are rebuilding the layout in the shop currently and I can work this right into a dead corner.

Thanks for posting what a great idea.

Is that the:

Matrix Horticulture 96"x96"x80"
That's the one.
__________________
WWUD? Think for yourself.
Reply With Quote
  #7  
Old 01-11-2018, 01:38 PM
Dan Vanantwerp
Guest
 
Posts: n/a
This looks fan-freaking-tastic

Am wondering if you could add a dehumidifier to keep the chemicals nice and dry. Dave mentions the issues he's had with water content and accurately weighing out ingredients. This might remove that variable.
Reply With Quote
  #8  
Old 01-11-2018, 02:54 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,790
Pete VanderLaan is on a distinguished road
It has a dehumidifier which costs as much to run as AC does. It's a very good idea. It would require one to not be a slob about it. I fail . I spill a lot too. The last thing I ever want to do is to clean the floor. Once a year. The worst chemical to try to keep is potassium carbonate. I put it in ziplocs as soon as I open a bag.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #9  
Old 01-11-2018, 06:19 PM
Dan Vanantwerp
Guest
 
Posts: n/a
Whoops...

"I also have a dehumidifier that keeps the RH right at 35%."

...missed that part!
Reply With Quote
  #10  
Old 01-11-2018, 06:57 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,790
Pete VanderLaan is on a distinguished road
Hey, Look! We use a lot of "hothands" back here in our gloves and boots. The big ones last 18 hours. I finally decided to test a simple chemical oxygen theory and as fast as I use some big ones and came inside, I put them in tight aluminum foil and they went cold instantly. Later in the day, I used them again and unwrapped them and they got hot again in a few minutes/ I did the horse maintenance number and re wrapped them for tomorrow.

Call me cheap but they are about .70 for the 18 hours and I use up to eight of them in each boot or glove. It adds up if you have to overpay for Venice.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #11  
Old 01-12-2018, 11:59 AM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,750
Jordan Kube is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
Hey, Look! We use a lot of "hothands" back here in our gloves and boots. The big ones last 18 hours. I finally decided to test a simple chemical oxygen theory and as fast as I use some big ones and came inside, I put them in tight aluminum foil and they went cold instantly. Later in the day, I used them again and unwrapped them and they got hot again in a few minutes/ I did the horse maintenance number and re wrapped them for tomorrow.

Call me cheap but they are about .70 for the 18 hours and I use up to eight of them in each boot or glove. It adds up if you have to overpay for Venice.
Brilliant!
__________________
WWUD? Think for yourself.
Reply With Quote
  #12  
Old 01-12-2018, 01:00 PM
Dave Bross Dave Bross is offline
Registered User
 
Join Date: Apr 2002
Location: Archer FL(near Gainesville)
Posts: 3,001
Dave Bross is on a distinguished road
Excellent!

Also reminds my twisted sense of humor of the bubble boy movie.


https://www.rottentomatoes.com/m/bubble_boy/
__________________
Art is not a thing...it's a way.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 03:08 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.