Casting a v belt pulley

Anyone cashed a v belt pulley? What method did you use? The v is a pain to make in a mold. Wax?.
Franklin
Reply With Quote
  #2  
Old 08-05-2017, 04:54 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,583
Pete VanderLaan is on a distinguished road
Buy it Franklin. This particular wheel is a bear to balance even if you can get the basic casting right. It would need some machining.. Some things are better not done. Tell us the bore size and the pulley size diameter. You may be able to simply find it in an auto wrecking place.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 08-05-2017, 10:27 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,751
Franklin Sankar is on a distinguished road
Thanks Pete. It's to use as a pulley for opening a door not for spinning so not too worried about balancing. I was curious as to how you could cast it. Looks very difficult.
Franklin
Reply With Quote
  #4  
Old 08-06-2017, 08:01 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,583
Pete VanderLaan is on a distinguished road
Make it out of wood then. A Circular piece of a hardwood ( or plywood). Then attach two more pieces on the outside of that a slightly larger diameter just enough so the cable cant slip over it. Drill a hole in the middle.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 08-06-2017, 10:48 AM
Steven O'Day Steven O'Day is offline
Registered User
 
Join Date: Jun 2002
Location: portland oregon
Posts: 301
Steven O'Day is on a distinguished road
It would involve sand casting in a multi-part mold and then like Pete said, machining and balancing.
Reply With Quote
  #6  
Old 08-06-2017, 12:23 PM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,400
Eben Horton is on a distinguished road
Take 2 coconuts. Cut them to get 2 quarter shapes and bolt them together. There's your v-belt wheel. I learned that from watching Gilligan's Island as a kid.
Reply With Quote
  #7  
Old 08-06-2017, 01:08 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,751
Franklin Sankar is on a distinguished road
Lol. Now I need a plan for reaching them.
Franklin
Attached Images
File Type: jpg image.jpg (47.5 KB, 32 views)
Reply With Quote
  #8  
Old 08-07-2017, 02:26 PM
Dan Vanantwerp Dan Vanantwerp is offline
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 254
Dan Vanantwerp is on a distinguished road
Ginger or Mary Ann?...or Jeannie?
__________________
My furnace setting: 2112
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 11:04 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.