shutting off the glory hole

I noticed on a recent thread that Pete was not in favor of shutting off an unused glory hole, and I'm interested to know the reasoning behind that.
In my shop, I put switches on both my glory holes that I can operate with my foot.
I'll light them both, a large one and a small one, and let them come to temperature. Then as I'm working, I'll start out in the small one till my piece outgrows it and I switch to the large one. At that point I'll shut off the small one, as I won't be needing it for twenty minutes or so. The door is shut, so it doesn't lose enough heat to take long in warming back up. Once the piece is finished and in the oven, I'll shut the door on the large hole and turn that off, having turned on the small one in preparation for starting the next piece. I'll turn on the large one long enough before needing it that it has ample time to get back to full temperature. it takes maybe a couple of minutes.
In my thinking, I'm not only saving fuel, but also keeping the shop cooler and quieter in the process. At the same time, I've learned not to trust my conjecture in the face of someone more knowledgeable.
Am I missing something here? I don't have to waste fuel waiting for the furnaces to come back to heat, and it doesn't seem like the refractory is suffering much from cycling, but again, I could be missing something important
Reply With Quote
  #2  
Old 11-13-2018, 07:28 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,097
Pete VanderLaan is on a distinguished road
To each their own. It sounds like you have a fiber gloryhole but it may be cast or brick.

When I was working in Shanghai, Wang Kai kept shutting off the glory hole if we had the work out on the bench. It drove me crazy. I never had the radiant heat I wanted from the front of the gloryhole. Eveline told him he had to stop.

I use a larger gloryhole than necessary so I don't have to consider stuff like that. There's a limit. We have two here, one about 12 inch and the other sixteen. These days the only one we use is the 16. I don't think there's any right or wrong way to do this stuff.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 11-13-2018, 10:55 AM
Scott Novota's Avatar
Scott Novota Scott Novota is offline
AbbyNormal User
 
Join Date: Jan 2004
Location: Pensacola Florida
Posts: 2,141
Scott Novota is on a distinguished road
Time vs. hassle is why I would not do this. If your time and hassle ratio is worth the cost savings who am I to tell you it is wrong?

I would look into exactly what you think your saving vs what you are actually saving. Start your day and mark your gas meter numbers down. Work as you normally would switching, waiting, and working our system.

Do it the next day but just use the larger of the two gloryholes.

Now take your bill and figure out what your cost is per unit and compare. See if your day to day change is worth the effort? Did you get and extra piece out by not switching around? Did you make better work by not having a distraction?

Eh, might be worth it but you will never know until you figure out what you may or may not be saving.

Me I just fire up one glory if I might be making larger work and the small one if I know I will be under 10 inches. Keeps things simple.
Reply With Quote
  #4  
Old 11-13-2018, 04:04 PM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,506
Eben Horton is on a distinguished road
the best way to save costs in the hot shop is to blow as much glass as possible until you just can't deal anymore, say 3 months straight and then shut the furnace off for a a few months.

I turn my hole off when I take a lunch break.

Something to consider is that a HOT hole can make things a lot faster to make as opposed to a colder hole. don't be a penny wise and a pound foolish.
__________________
<eben epoiese>
Reply With Quote
  #5  
Old 11-13-2018, 07:29 PM
Philip Yamron Philip Yamron is offline
Registered User
 
Join Date: Jul 2012
Location: Ann Arbor, MI
Posts: 76
Philip Yamron is on a distinguished road
Why not just put a 2nd set of doors on the larger GH. Second set having a smaller opening. Then 1 hole used and you just leave the smaller doors open as your work increases in size.
Reply With Quote
  #6  
Old 11-13-2018, 08:16 PM
Josh Bernbaum Josh Bernbaum is online now
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 611
Josh Bernbaum is on a distinguished road
I'd agree with Scott. You really should meter your usage and the numbers
won't lie about whether this method of the on/off with the two holes is more efficient or not. Maybe it's similar fuel use either way and then you choose what's more convenient or easier. Won't know till you know.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #7  
Old 11-14-2018, 06:43 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,097
Pete VanderLaan is on a distinguished road
mine keeps the studio warm. A biggie.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 11-24-2018, 07:08 AM
bob gent bob gent is offline
Registered User
 
Join Date: Oct 2016
Location: lawrence, ks
Posts: 9
bob gent is on a distinguished road
thanks for the feedback. I've just moved to the country and need to put up a building to house the shop, so there's a lot of chances to rebuild stuff differently. Maybe I ought to think about putting new doors on the big glory hole. I haven't ever made a hole with multiple sized doors. maybe now's the time
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 08:22 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.