Neodymium effecting expansion?

So I was able to get a good price on some chemicals that Mr. Dudley Gibberson was interested in getting rid of recently. It was a pleasure getting to see his shop in the woods in NH and what he'd been doing there figuring out glass melting stuff since before almost anyone else in our studio glass movement. One of the things he parted ways with was a bunch of Neodymium. I haven't done any melts with this colorant yet, but I'd like to add some in with a phosphate mix I'll do tomorrow. After reading some of Weyl on this, and wanting a somewhat stronger effect from the Neo, I thought I'd go with a 4% addition. Weyl suspected that the "Alexandrite" glass produced by Moser in Czech. was a 4%, and upon looking at images online of their antique (and maybe still current?) products, I think that's a nice coloration. So question then is, since I don't see it listed on the two spreadhseets I have, will this have any significant effect on expansion, and if so, up or down? Just curious to know if I should plan on compensating in my mix. Thanks
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:56 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.