Old 04-13-2019, 02:09 PM
Ron Mynatt Ron Mynatt is offline
Registered User
 
Join Date: Apr 2008
Location: Springdale Arkansas
Posts: 164
Ron Mynatt is on a distinguished road
blown glass /neon

I have seen a neon art piece using a soda lime blown glass form .It has been a few years back so I can't find it now . A local neon artist has asked if it could be done .Any suggestions on how this could be done ?
Reply With Quote
  #2  
Old 04-13-2019, 02:41 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 552
Shawn Everette is on a distinguished road
It's tricky, but you can do it. Basically you need to attach a tubulated electrode to your piece while you've got it on the pipe, then box it almost immediately, and take it through the anneal cycle. Once it's cool you can attach the tubulation to the electrode and have it lead out to the pump setup. It's advisable to process the electrode though an induction heater before doing this if possible. Test the piece for leaks. At this point you are ready to process the piece by taking it back up to annealing and back down under vacuum, effectively removing all contaminants. Once you're about 100f, proceed to fill with gas of choice and tip off the electrode.

In theory there are a few steps you could skip, but would lead to possible contamination and give lesser quality of light or shorten the lifespan.
Reply With Quote
  #3  
Old 04-13-2019, 05:45 PM
Rick Kellner Rick Kellner is online now
Registered User
 
Join Date: Jan 2004
Location: Hillsboro, OR
Posts: 200
Rick Kellner is on a distinguished road
Occasionally, you will also see such pieces made without electrodes. By using a special base with power supply that emits a high frequency energy field, it is possible to light up a piece wirelessly. You would, however, still need to tubulate the piece with a section of 5 or 6 mm diameter tubing in order to evacuate the piece while baking out the impurities, then backfilling on a manifold with your noble gases of choice. The only missing step would be the induction heating of the electrode(s) to incandescence.

If you are crafty enough with methodical pre-heating, and flame annealing, you can get away without many of the steps above by attaching electrodes (or tubulating) with a torch from a cold start, on a previously annealed piece of glass. Having a particularly thin wall on your blown piece is likely to factor in to your success with the endeavor.

In my experience, some of the plasma art and single electrode work seems to be a bit more forgiving in terms of processing purity, compared to traditional luminous tubing that is processed by electrical bombardment with a large high voltage transformer.
Attached Images
File Type: jpg IMAG2760.jpg (17.8 KB, 21 views)
Reply With Quote
  #4  
Old 04-13-2019, 06:07 PM
Rick Kellner Rick Kellner is online now
Registered User
 
Join Date: Jan 2004
Location: Hillsboro, OR
Posts: 200
Rick Kellner is on a distinguished road
If you want to see a compendium of state of the art work in this area, consider checking out the instagram page for taminglightning. The creator might also have a podcast, but I am not familiar with it. Anyway, many artists are featured there, and you can see numerous examples of neon work originating in the hot shop.
Reply With Quote
  #5  
Old 04-13-2019, 06:12 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 552
Shawn Everette is on a distinguished road
Rick is correct that a proximity field set up will generally be easier to get processed, and not need as much purity, but you sacrifice a significant amount of light, and make art that's potentially problematic for pacemakers. I've got 8 year old pieces that are still going that are annealed, tubulated, and pumped; but they're best visually in dim rooms.

Processing purity in traditional neon is more important because there is enough energy going through the tube to cook the dirt and start to decrease the pressure of the vacuum, eventually leading to failure. Single electrode some what less important, no electrode even less. Never the less, properly processed glass is going to lead to lights that will out last you.

It would be hard to say the best way to attack this without knowing more about the object, or how you plan to display it.
Reply With Quote
  #6  
Old 04-13-2019, 06:16 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 552
Shawn Everette is on a distinguished road
Also check out PAA, believe it was started by Wayne Stratman who is one of the godfathers of alternative process.
Reply With Quote
  #7  
Old 04-14-2019, 01:37 PM
Ron Mynatt Ron Mynatt is offline
Registered User
 
Join Date: Apr 2008
Location: Springdale Arkansas
Posts: 164
Ron Mynatt is on a distinguished road
Thanks for the information .This seems involved but it also seems like is doable. .
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 11:15 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.