System 96 + Glasma mismatch

I had a very interesting failure recently and I thought Id post the story here. Maybe it will sound familiar to somebody or maybe it will save someone some trouble. I made murrine by fusing stacks of System 96 sheets and cutting the resulting blocks into squares. The murrine were 6 mm thick and I framed them with strips of black and white. After rolling it up I covered it with one gather of Glasma.

A week after making, I did a flat grind on the bottom and put it on a shelf. Two weeks after making, it spontaneously exploded. From the other side of the house, it sounded like somebody dropped a pile of dishes.

The obvious suspect is 12 different colors of System 96 but I have had a couple of failures using Reichenbach colors with Glasma while I didnt have a single one in my previous studio using Cristalica. I realize that Im mixing some unusual things but if anyone has any ideas, Id like to hear them.
Attached Images
File Type: jpg Fused murrines.jpg (31.7 KB, 71 views)
File Type: jpg Broken Fused murrines.jpg (36.1 KB, 79 views)
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 11:25 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.