Hi Everyone!

New here, but been reading for a few months.
I come from the Boro glass world. Ive been working with glass for 18years, and did 4 years of Hot Shop work a while ago and im setting up to get back into it as i miss it... im old school and I love forum format, less annoying that facebook, and more indepth.

I will run for now the small hot shop with the 2 Skutt Furnace i was using to melt borosilicate, using 30 and 60pounds crucible.


As im working on getting the new 800sqf ready for the hot shop, im really debating about the best way to finish the floor on it.

It is a thick heated radiant Slab , with the actual finish being hand trowel.

Im wondering if i should leave it as is or acid wash and seal as i usually do , or else ?... most shop i saw had a nice finished flooring made with the helicopter machine or flat grounded by sander... mine if more ruff..

Since we will most obviously drop a bunch on glass on it, im wondering about offgazing/burning the stain or the sealer i would put on it , but also that would generate toxic gases while burning etc... I dont care about burn mark, but more about the toxic side of it...
but leaving it as is might imply more dust, more porous, etc...

if you guys have any input on this it would be greatly appreciated,

sorry if my english isnt always perfect as my first language is French.. (Quebec)

Thanks !

Loc
Reply With Quote
  #2  
Old 04-14-2020, 07:36 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,987
Pete VanderLaan is on a distinguished road
Mine ran a polisher until they ran out of fuel and it was sealed with Thompson's water seal.

I've had broom surface in the past and regretted it.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 04-14-2020, 11:10 PM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,549
Rich Samuel is on a distinguished road
Is there a drain? If not, won't the radiant slab make installing one tricky?
Reply With Quote
  #4  
Old 04-15-2020, 07:17 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,987
Pete VanderLaan is on a distinguished road
I had a drain in my slab. I used it and it clogged permanently. Bullseye had floor drains and in the end game had to clean out the Portland Storm drain system. Better to use oiled sawdust for cleanup.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 04-15-2020, 08:45 AM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 652
Art Freas is on a distinguished road
Done a lot of building and a lot of concreate work. I agree with Pete, no broom finish, will trap a lot of dirt and glass dust. My one concern is with the underfloor radiant heat. If it is the plastic pipe in the concrete I am not sure how that would behave under the furnace. I would check with the manufacturer and make sure there is some heat barrier between the furnace in the floor. If it is a fluid system it may transfer heat the the rest of the shop when it is not running even in summer. Over time that part of the floor picks up a lot of heat. Not sure how the pipe would behave. For a floor drain there are specialized traps but you have to be diligent about cleaning them. If you do put in a drain go oversized both in pipe size and trap size. Also make sure you have a good cleanouts in the pipe run.
Reply With Quote
  #6  
Old 04-15-2020, 08:54 AM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 685
Josh Bernbaum is on a distinguished road
I caught my concrete guy just getting ready to pour some sealant on the floor just after he cast it and 'helicopter' machined it here years ago. I asked "what's in that bucket?" He said it was some plastic-y type sealant that would make the floor look good. I'm glad I caught him in time and he didn't pour it. I could only imagine that anything hot that dribbled on the floor would make that burn and maybe leave marks. 13 years later, my floor looks fine to me, even without a sealant.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #7  
Old 04-15-2020, 09:57 AM
Max Epstein Max Epstein is offline
Registered User
 
Join Date: Sep 2016
Location: Tallahassee, FL
Posts: 383
Max Epstein is on a distinguished road
Not germaine to the conversation, but heated floors are the shit. Had them up in Alaska and made all the difference.
Reply With Quote
  #8  
Old 04-15-2020, 10:24 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,987
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Josh Bernbaum View Post
I caught my concrete guy just getting ready to pour some sealant on the floor just after he cast it and 'helicopter' machined it here years ago. I asked "what's in that bucket?" He said it was some plastic-y type sealant that would make the floor look good. I'm glad I caught him in time and he didn't pour it. I could only imagine that anything hot that dribbled on the floor would make that burn and maybe leave marks. 13 years later, my floor looks fine to me, even without a sealant.
****
The purpose of the sealant ( Thompson's) is actually to help the concrete cure slowly. I don't get any residue burning off my floor.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #9  
Old 04-15-2020, 03:08 PM
Victor Chiarizia Victor Chiarizia is offline
Registered User
 
Join Date: Sep 2005
Location: fairview, NC
Posts: 578
Victor Chiarizia is on a distinguished road
i stained and sealed my floor 15 years ago and it still looks pretty good. pex tubes are good to ~180deg F so i don't think there's an issue. had them in my shop in CT and the floors were wonderful to stand on bare footed. have them in my house i built here in NC too. best heat in the world. vic

oh....power trowed is my finish of choice although they can be slippery when wet if the guy trowels them too well. stains are fantastically beautiful and you can apply them yourself.
Reply With Quote
  #10  
Old 04-15-2020, 03:13 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Triggered
 
Join Date: Jan 2007
Location: Aarde
Posts: 2,225
Greg Vriethoff is on a distinguished road
I think the sealant that Josh is referring to might be a coating rather than concrete sealer. A friend of mine here in Charlotte has been building a studio (not a glass person, but a ceramist) and used an epoxy-type coating. These are good for easy maintenance, but yeah, you don't want to be dribbling hot glass on 'em.
Reply With Quote
  #11  
Old 04-15-2020, 05:33 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 652
Art Freas is on a distinguished road
Quote:
Originally Posted by Victor Chiarizia View Post
i stained and sealed my floor 15 years ago and it still looks pretty good. pex tubes are good to ~180deg F so i don't think there's an issue. had them in my shop in CT and the floors were wonderful to stand on bare footed. have them in my house i built here in NC too. best heat in the world. vic

oh....power trowed is my finish of choice although they can be slippery when wet if the guy trowels them too well. stains are fantastically beautiful and you can apply them yourself.
Good to hear on the tubes, I honestly never had anyone have any thing as hot as a furnace above them. Had the concrete folks put them in the wrong place on a habitat build and we couldn't shoot the plates in, had to use some nasty glue for the interior walls on the slab.
Reply With Quote
  #12  
Old 04-21-2020, 12:21 AM
Hugh Jenkins Hugh Jenkins is offline
Registered User
 
Join Date: Sep 2006
Location: Honoka'a, HI
Posts: 1,000
Hugh Jenkins is on a distinguished road
If you still can, make all surfaces drain to the walls and put in scuppers so you can hose out. I have had some issues at the school with smooth floors and spilled water. I did do broom finish on my current shop extension and it requires vacuuming rather than sweeping for real cleaning.
__________________
Aloha, Hugh
Reply With Quote
  #13  
Old 04-25-2020, 01:34 PM
Paul Thompson Paul Thompson is offline
Registered User
 
Join Date: Apr 2007
Location: Hygiene CO
Posts: 197
Paul Thompson is on a distinguished road
Quote:
Originally Posted by Hugh Jenkins View Post
If you still can, make all surfaces drain to the walls and put in scuppers so you can hose out. I have had some issues at the school with smooth floors and spilled water. I did do broom finish on my current shop extension and it requires vacuuming rather than sweeping for real cleaning.
Wouldn't troughs along the walls be hidden under cabinets, shelves and equipment?
__________________
"You don't have to be a very good glassblower when you can fix stuff" -- Richard Royal
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 05:06 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.