pastoralli secrets needed

so can anyone help with sticking murrini on a ceramic pastorali please. i'm using a corundum plate and the murrini are sticking to the wash thats on the plate. i'm trying to get a full fuse/tack to roll up the glass onto a collar. i have kiln wash and bentonite available. i think there's too much wash on the plate first off. we heat and rotate the plate several times before the rollup. thoughts? vic
Reply With Quote
  #2  
Old 12-20-2017, 08:58 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,402
Eben Horton is on a distinguished road
15 years ago I bought some cast iron plates. Not once have I ever had a problem with sticking, spalling or anything. Ceramic plates get hot quick, are pourus and are brittle. The only upside I can see is that they are light.

That said. Have you tried ceramic paper? I think that is bomb proof, but dusty.
Reply With Quote
  #3  
Old 12-20-2017, 09:17 AM
Marty Kremer Marty Kremer is online now
Registered User
 
Join Date: May 2004
Location: North Yarmouth ME
Posts: 446
Marty Kremer is on a distinguished road
Have you tried Bullseye's kilnwash?
Reply With Quote
  #4  
Old 12-20-2017, 10:13 AM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 512
Art Freas is on a distinguished road
Most of the time sticking is because the wash was put on too thick. The wash should be really thin when put on, really thin, like watered down milk. And lots of coats.
Reply With Quote
  #5  
Old 12-20-2017, 11:05 AM
David Patchen's Avatar
David Patchen David Patchen is offline
Registered User
 
Join Date: Sep 2005
Location: San Francisco, CA
Posts: 1,863
David Patchen is on a distinguished road
Of course, there's lots of ways to skin this cat, but once you get it dialed, you'll rarely run into this problem again--until the plate needs re-washing. Here's blog post I did on this (since I get asked it a lot).

http://davidpatchen.com/content/how-...ne-and-murrine

Hope this helps. And keep your heats short!
Reply With Quote
  #6  
Old 12-20-2017, 11:58 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,598
Pete VanderLaan is on a distinguished road
Well written David. I have put a link to your site in Antiques and Classics on the subject unless you object. If so send Louis the Leg breaker to my winter quarters.

I will print it out if you don't mind, attribution of course.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 12-20-2017, 04:20 PM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 582
Josh Bernbaum is on a distinguished road
For murrini, I think it helps to torch the glass tiles from above between heats to help the heat build in the center tiles and also to prevent the plate from overheating. Also flipping the whole sheet like a pancake (after it's fused at least a bit) can help. When I worked for you years ago Victor, I remember your GH ran quite hot. While I think that helps a lot of things go quicker, I also think that may contribute to the tiles sticking to your plate..
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #8  
Old 12-20-2017, 07:41 PM
Victor Chiarizia Victor Chiarizia is offline
Registered User
 
Join Date: Sep 2005
Location: fairview, NC
Posts: 550
Victor Chiarizia is on a distinguished road
interesting you remember that Josh. i do run my hole a bit hot. thanks for the sticky pete and david. vic
Reply With Quote
  #9  
Old 12-21-2017, 08:06 AM
Kenny Pieper Kenny Pieper is offline
Registered User
 
Join Date: Feb 2003
Location: Burnsville N.C.
Posts: 818
Kenny Pieper is on a distinguished road
I was shown and use an almost opposite approach to what David has explained. I like for the wash to be really thin on the surface. To this end I soak the shelf first so that when I apply the wash it doesn't dry up right away on the surface. This also allows the wash to soak into the poors of the shelf which in my view is a plus. The wash is a really thin mixture of equal parts silica, alumina hydrate, and E.P.K. clay with water added. Just after applying the wash while it is still wet it hardly looks like anything is on it. After drying it in the garage it is fired in the gloryhole and by this time there is a thin layer of the white wash visible on the surface. I usually give it a light wipe with a rag to dust off any loose particles on the surface before the first use. It will last 6 months to a year with regular use. Before the next application I will grind off the surface of the shelf with the diamond flat grinder.
Now I am not saying this is any better just different.
Reply With Quote
  #10  
Old 12-23-2017, 12:23 PM
David Patchen's Avatar
David Patchen David Patchen is offline
Registered User
 
Join Date: Sep 2005
Location: San Francisco, CA
Posts: 1,863
David Patchen is on a distinguished road
Quote:
Originally Posted by Kenny Pieper View Post
I was shown and use an almost opposite approach to what David has explained. I like for the wash to be really thin on the surface. To this end I soak the shelf first so that when I apply the wash it doesn't dry up right away on the surface. This also allows the wash to soak into the poors of the shelf which in my view is a plus. The wash is a really thin mixture of equal parts silica, alumina hydrate, and E.P.K. clay with water added. Just after applying the wash while it is still wet it hardly looks like anything is on it. After drying it in the garage it is fired in the gloryhole and by this time there is a thin layer of the white wash visible on the surface. I usually give it a light wipe with a rag to dust off any loose particles on the surface before the first use. It will last 6 months to a year with regular use. Before the next application I will grind off the surface of the shelf with the diamond flat grinder.
Now I am not saying this is any better just different.
I love this--it's the perfect example that there's no *one right* way to do so many things in glass.
Reply With Quote
  #11  
Old 12-23-2017, 12:24 PM
David Patchen's Avatar
David Patchen David Patchen is offline
Registered User
 
Join Date: Sep 2005
Location: San Francisco, CA
Posts: 1,863
David Patchen is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
Well written David. I have put a link to your site in Antiques and Classics on the subject unless you object. If so send Louis the Leg breaker to my winter quarters.

I will print it out if you don't mind, attribution of course.
With the additional eyeballs, I reviewed it and recently edited for greater clarity. If you printed it, get a fresh one...
Reply With Quote
  #12  
Old 12-23-2017, 01:04 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,598
Pete VanderLaan is on a distinguished road
I don't see any edit in either of the two site sources on craftweb using the link you provided. If someone clicks that link, do they get the edited version?
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:12 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.