Concentrator pressure relief valve

Does anyone know if the oxygen concentrator have a pressure relief valve so if I shut off the torch the pressure is released. Ie no back pressure.
Franklin
Reply With Quote
  #2  
Old 11-27-2019, 10:10 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 552
Shawn Everette is on a distinguished road
Generically it should do it on it's own. It isn't really much of a compressor, so it doesn't actually store anything thing in the unit and will continue to run. There shouldn't be enough back pressure to cause harm, but you're losing time from it's life span.
Reply With Quote
  #3  
Old 11-27-2019, 12:10 PM
Ted Trower's Avatar
Ted Trower Ted Trower is offline
Registered User
 
Join Date: Apr 2002
Location: Ann Arbor, Michigan
Posts: 542
Ted Trower is on a distinguished road
Shutting of the flow from a concentrator will cause an alarm to sound. Don't know if it will harm the compressor but the alarm certainly is annoying. I just left my O2 valve open. Was using a surface mix torch so no real problem doing that.
__________________
"It appears to me that glass men are the most given to drunkeness of any class of men I know" Peter Burt, recruiter in Europe, in a letter to Deming Jarves of the Boston and Sandwich glass company. -1826
Reply With Quote
  #4  
Old 11-28-2019, 07:54 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,968
Franklin Sankar is on a distinguished road
I was thinking about if you want to adjust the oxygen you have to throttle it back .
Do you ever have to throttle back the oxygen other than at start up. What pressure do you use on your torch? At 20 psi the torch screams.
Anyone knows what pressure this torch works with? I got it a while ago . It roars like a lion. It also sings.
Franklin
Attached Images
File Type: jpg image.jpg (43.4 KB, 22 views)
Reply With Quote
  #5  
Old 11-28-2019, 07:59 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,968
Franklin Sankar is on a distinguished road
Shaun I am afraid to ask but any guess on how bad the wear will be. If itís slow then that is good.
Franklin
Reply With Quote
  #6  
Old 11-28-2019, 09:23 AM
Brian Graham's Avatar
Brian Graham Brian Graham is offline
Registered Abuser
 
Join Date: Mar 2004
Location: Akron - Ohio
Posts: 539
Brian Graham is on a distinguished road
Insert a T in the line with a valve to blow it off if you are worried. I always let mine escape because I have an old Nortel Major / Minor burner with two torch heads.
__________________
The revolution will not be televised.
Reply With Quote
  #7  
Old 11-28-2019, 11:16 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,968
Franklin Sankar is on a distinguished road
Thanks. That is the problem with my torch. The one lever turns on either the rings or the center . I am not sure I can turn on both at the same time. I will put a pressure relief valve if there is none. Arggg now to find one. Or maybe a bleed valve.
Franklin
Reply With Quote
  #8  
Old 12-01-2019, 02:42 AM
David Hopman David Hopman is offline
Registered User
 
Join Date: Mar 2009
Location: Sutter Creek, CA
Posts: 441
David Hopman is on a distinguished road
Just leave the oxygen on the torch open all the time so the concentrators do not ever have back pressure. It can ruin them.
Reply With Quote
  #9  
Old 12-01-2019, 04:27 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,968
Franklin Sankar is on a distinguished road
Thanks. How about if I add a bleed off valve, fully open the oxygen on the torch .
Then use the bleed off valve to control the oxygen flow. Open the bleed reduce the flow to the torch.
Franklin

Last edited by Franklin Sankar; 12-01-2019 at 06:59 AM.
Reply With Quote
  #10  
Old 12-01-2019, 07:28 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 769
Michael Ahlefeldt-Laurvig is on a distinguished road
I dont know the first thing about oxygen concentrators or torches, but would it be possible to run the eccess into a cheap say plastic pool for kids, and then throw a tire or something on it to press it out?
Reply With Quote
  #11  
Old 12-05-2019, 03:09 AM
David Hopman David Hopman is offline
Registered User
 
Join Date: Mar 2009
Location: Sutter Creek, CA
Posts: 441
David Hopman is on a distinguished road
I do all of the torch adjustment with the propane, not the oxygen. It is pretty much wide open all the time. The wife does something similar on her lampworking torch, and only turns down the oxygen when she needs a really fine flame, but she opens the outer ring oxygen to prevent back pressure. She is doing huge 104 lampworked focal beads that take up to 2 hours and is using a OGSI 20 unit.
Reply With Quote
  #12  
Old 12-06-2019, 08:42 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,968
Franklin Sankar is on a distinguished road
How do you light it with the oxygen wide open. Does it pop back. I get a big flame with the oxy wide open. Great for big things.
Franklin
Reply With Quote
  #13  
Old 12-09-2019, 02:49 AM
David Hopman David Hopman is offline
Registered User
 
Join Date: Mar 2009
Location: Sutter Creek, CA
Posts: 441
David Hopman is on a distinguished road
No pop at all. Just barely crack the propane and light it, then adjust the propane.
Reply With Quote
  #14  
Old 12-09-2019, 09:00 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,858
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Michael Ahlefeldt-Laurvig View Post
I dont know the first thing about oxygen concentrators or torches, but would it be possible to run the eccess into a cheap say plastic pool for kids, and then throw a tire or something on it to press it out?
****
That sounds to me like an extreme fire hazard.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #15  
Old 12-09-2019, 04:35 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 995
Sky Campbell is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
****
That sounds to me like an extreme fire hazard.
Yes but oxygen isnít flammable. Yes I know unsafe storage.


People commonly use oil less compressors matched to the bunch of concentrator total output for low pressure high volume systems. Just up to a few hundred psi so no chance of friction caused fires in the presence of oil. The bigger the tank the better new propane tanks or new air compressor tanks seem to be a good choice. Iíve seen some really scary oxygen containment systems.
Reply With Quote
  #16  
Old 12-09-2019, 07:04 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 769
Michael Ahlefeldt-Laurvig is on a distinguished road
Yea your right Pete, Ive only had high pressure bottle as in welding bottles, as I said no experience in torches or concentrators. Just thinking aloud
Reply With Quote
  #17  
Old 12-10-2019, 10:49 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,858
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Sky Campbell View Post
Yes but oxygen isn’t flammable. Yes I know unsafe storage.

****
I used to be in the business of responding to bad thinking and supressing the results of it. Oxygen doesn't burn by itself but it promotes ignition sources and vigourously supports combustion. Ask the Apollo astronauts that died in their capsule. The reasons why nitrates are clearly marked "Oxidizers" and have restricted storage and shipping requirements are clear. The limits of what can be stored on your site are clear. Oxygen is sticky stuff. It clings to clothing, drapes, chairs and it just needs a spark.
If you know about unsafe storage yet still do it, you just haven't experienced it firsthand yet.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #18  
Old 12-10-2019, 12:39 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 995
Sky Campbell is on a distinguished road
Knowing unsafe storage and actually doing it are two different things. I like to keep my oxygen in a liquid state as much as possible in a approved and certified dewar.

One of the first high volume low pressure oxygen systems was pioneered by a lamp worker. The one I saw was built storing oxygen in a non aproved bladder and compressing the bladder for pressure. This experiment pushed the idea forward and has been reengineered by many. Everything starts somewhere.

And oh yes I have seen what oxygen can do in saturation. Scary stuff. My best advise is to understand your freedom stops when it infringes on someone elseís. This means not putting firefighters or neighbors at risk.

I would like to see cost analysis of feeding pure oxygen into the fuel stream on the glory. These 5 and 10 liter machines use hardly any power and can be found for free all over the states.
Reply With Quote
  #19  
Old 12-10-2019, 02:11 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,858
Pete VanderLaan is on a distinguished road
Knowing and doing..

I recall where the reality show "Forged in Fire" had someone watching it who managed to burn down his city block in New York having been inspired by the show, so I have a tendency to consider the lower common denominators on the board of which tons are simply lurking. I try not to take quite a few things for granted.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 01:20 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.