Fuji PXR3 controller?

Was wondering if anyone had a trick to resetting this controller. I had a power outage and restarted my hot furnace. Seemed to run through the ramp sections OK until it got to the 5th ramp which I had set to hold the working temp 2170. So as soon as it hits this temp it goes directly to the shut down program 6th ramp. I did not change anything so something must have been reset. tried to find a setting that would allow unlimited time once working temp is achieved, but all the manuals have you set a ramp time with a max 99hrs 59min. Any ideas would be appreciated. Thanks Paul

labrieglass.com
Reply With Quote
  #2  
Old 05-03-2018, 01:57 PM
Richard Huntrods's Avatar
Richard Huntrods Richard Huntrods is offline
Registered User
 
Join Date: Aug 2003
Location: Vancouver Island
Posts: 1,176
Richard Huntrods is on a distinguished road
Thumbs up

Quote:
Originally Posted by Paul Labrie View Post
Was wondering if anyone had a trick to resetting this controller. I had a power outage and restarted my hot furnace. Seemed to run through the ramp sections OK until it got to the 5th ramp which I had set to hold the working temp 2170. So as soon as it hits this temp it goes directly to the shut down program 6th ramp. I did not change anything so something must have been reset. tried to find a setting that would allow unlimited time once working temp is achieved, but all the manuals have you set a ramp time with a max 99hrs 59min. Any ideas would be appreciated. Thanks Paul

labrieglass.com
Is this the original PXR3 with 2 x 4 step programs which can be combined into 1 x 8 steps, or a newer one with more steps per program?

I ask because if you are using all 8 steps in one program, then yes - it will go from step 5 to step 6 when the timers say.

There are 3 parameters per program step: set point, ramp time and soak time.

When you say step 6 is shutdown, do you mean you actually shut things down using a ramp and setpoint, or is step 6 just the default values? Because if step 6 has defaults, then it should hold the step 5 setpoint indefinitely.

Default values for the PXR3 are 32, 0.0 and 0.0 (assuming temp in F). If step 6 is not these defaults, then step 6 will run as soon as the ramp time for step 5 is done.

Here's my typical blowing program, which starts with the furnace idling at 1900F:

SU-1 temp1 2100.00
RN1R ramp1 2.00
RN1S soak1 0.10

SU-2 temp2 32.00
RN2R ramp2 0.00
RN2S soak2 0.00

SU-3 temp3 32.00
RN3R ramp3 0.00
RN3S soak3 0.00

SU-4 temp4 32.00
RN4R ramp4 0.00
RN4S soak4 0.00

It's a simple program for sure, but it ramps the furnace from current temp (1900F) to 2100F over 2 hours, then soaks for 10 min. Because step 2 is defaults, it holds 2100F until I manually switch the program off, after which it defaults back to the current manual setpoint, which in my case is 1900F.

My batch cook program is in steps 5-8 but is similar.

I did find that you need a non-zero soak time for things to work as expected, so I just arbitrarily chose 10 min (0.10) and that works.
Reply With Quote
  #3  
Old 05-03-2018, 03:04 PM
Paul Labrie Paul Labrie is offline
Registered User
 
Join Date: Jan 2010
Location: Richland, WA
Posts: 26
Paul Labrie is on a distinguished road
Thanks Richard seems to be working
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On
Forum Jump


All times are GMT -5. The time now is 06:11 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.