CraftWEB Hot Glass Talk  

Go Back   CraftWEB Hot Glass Talk > Hot Glass > General Hot Glass Discussion

Reply
 
Thread Tools Display Modes
  #1  
Old 07-25-2020, 11:08 AM
Paul Thompson Paul Thompson is offline
Registered User
 
Join Date: Apr 2007
Location: Silver Spring MD
Posts: 201
Paul Thompson is on a distinguished road
"Alexandrian" glass confirmed by hafnium isotopes

(Link to article)

Abstract

Archaeological glass contains information about the movement of goods and ancient economies, yet our understanding of critical aspects of the ancient glass industry is fragmentary. During Roman times, distinct glass types produced in coastal regions of Egypt and the Levant used evaporitic soda (natron) mixed with Nile-derived sands. In the Levant, furnaces for producing colourless Roman glass by addition of manganese have been uncovered, whereas the source of the desirable antimony-decolourised Roman glass remains an enigma. In the Edict of Diocletian, this colourless glass is listed as “Alexandrian” referring to Egypt, but its origin has been ambiguous. Previous studies have found overlapping strontium and neodymium isotope ratios for Levantine and Egyptian glass. Here, we confirm these findings and show for the first time, based on glasses from the ancient city of Gerasa, that hafnium (Hf) isotopes are different in Egyptian and Levantine natron glasses, and that Sb Roman glass is Egyptian. Our work illustrates the value of Hf isotopes in provenancing archaeological glass. We attribute the striking difference in Hf isotopes of Egyptian versus Levantine glasses to sorting of zircons in Nile sediments during longshore drift and aeolian transport along the south-eastern Mediterranean coast leaving behind a less juvenile fraction.
__________________
"You don't have to be a very good glassblower when you can fix stuff" -- Richard Royal
Reply With Quote
  #2  
Old 07-25-2020, 05:47 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,289
Pete VanderLaan is on a distinguished road
we should not leave out effusive bullshit from the northern Hemisphere. It's had a permanent effect.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 07-25-2020, 11:25 PM
John Croucher's Avatar
John Croucher John Croucher is offline
Registered User
 
Join Date: Jul 2003
Posts: 67
John Croucher is on a distinguished road
It's interesting that, just as now in the 21st century glassblowers want to buy cullet, no latter how far it's got to be transported, so did glassmakers in Roman empire times. Most glass shops bought color and cullet from only 2-3 sources in the Levant and Egypt. The vessel makers rarely made their own glass.
The cullet was mostly melted close to good glass sands in large tanks. Very large tanks. The furnaces found at Bet Eli'ezer near Haifa in modern day Israel for instance, melted 8-10 tonne slabs of glass in situ and then the furnace was knocked down and the glass broken up into chunks which were shipped all over the Mediterranean.
Reply With Quote
  #4  
Old 07-26-2020, 11:00 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,289
Pete VanderLaan is on a distinguished road
So, somewhere out there was "The Tigris and Euphrates" Color rod company. Who knew?

I am continually amazed at how far melters would go and how they knew in that time period what was really important.

Stibnite? Really, how did they ever know. They were going to NE Turkey and to Iraq to get it. (Stibnite yields Antimony) . I have several Corning publications on ancient glass analysis and its simply remarkable how well balanced those ancient glasses were.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 07-26-2020, 12:14 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 600
Charles Friedman is on a distinguished road
If you are interested in the history of glass. This is a good read on old glass making and it's history. "Glassmakers: An Odyssey of the Jews : The First Three Thousand Years" by Samuel Kurinsky.
same with "Conciatore" The life and Times of 17th C Glassmaker - Antonio Neri. He printed the first book on glassmaking.

PS
I have missed doing glass so much I have resorted to "Mini chocolate-chips- roll-ups on a roasted marshmallow".
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
  #6  
Old 07-27-2020, 06:42 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 722
Art Freas is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
So, somewhere out there was "The Tigris and Euphrates" Color rod company. Who knew?
Phillipus of Olympus Vitreis Quis Color Virga?
Reply With Quote
  #7  
Old 07-27-2020, 07:57 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,289
Pete VanderLaan is on a distinguished road
Cheap imitator!!

John and I are starting to go around on the very subject. I love talking to John. If it's affordable, find "glass of the Alchemists" which Corning produced as a coffee table book about 20 years ago, maybe longer.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 07-27-2020, 07:59 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,289
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Charles Friedman View Post
If you are interested in the history of glass. This is a good read on old glass making and it's history. "Glassmakers: An Odyssey of the Jews : The First Three Thousand Years" by Samuel Kurinsky.
same with "Conciatore" The life and Times of 17th C Glassmaker - Antonio Neri. He printed the first book on glassmaking.

PS
I have missed doing glass so much I have resorted to "Mini chocolate-chips- roll-ups on a roasted marshmallow".
****
Thanks Charles, I have Neri but the other has been elusive at a fair price so far.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #9  
Old 07-28-2020, 12:34 PM
Tom Fuhrman Tom Fuhrman is offline
Registered User
 
Join Date: Apr 2002
Location: Lakeland, Florida
Posts: 1,480
Tom Fuhrman is on a distinguished road
I remember when Kurinsky gave a presentation at a GAS conference on his book. very interesting.
Reply With Quote
  #10  
Old 07-28-2020, 06:04 PM
Hugh Jenkins Hugh Jenkins is offline
Registered User
 
Join Date: Sep 2006
Location: Honoka'a, HI
Posts: 1,010
Hugh Jenkins is on a distinguished road
I got a copy of Kurinsy several years ago for almost the cost of shipping. It is a deadening read actually.Three months of self isolation and still not done. Three or four pages at a time is enough. But recalling his GAS presentation almost accusing everyone in the audience of intentional ignorance, it is interesting to read the historical information, much of which has been there, at least being compiled in readable form. Our adulation of Venice and the prominently advertised Egypt-ology, has overshadowed most of what came before that. Historical record was scarce 3000 years ago.
This story almost excludes the sociopolitical (ie warfare, conquest) that was coincident and makes it a little hard to overlay with the world history we were all taught, but puts some context into why glass was slow compared to ceramics, bronze and iron around the world. The pyrotechnology had to develop with wood as the major fuel.
__________________
Aloha, Hugh
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 07:23 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.