Sealing Brick Ceiling

I'm getting a small clamshell oven for roll-ups and whatnot. Trying to prevent IFB particles from falling onto the glass when opening- What can I coat the bricks with, to seal the surfaces?
Reply With Quote
  #2  
Old 11-16-2017, 04:37 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,573
Jordan Kube is on a distinguished road
Replace with fiberboard.
__________________
WWUD? Think for yourself.
Reply With Quote
  #3  
Old 11-16-2017, 05:28 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 19,829
Pete VanderLaan is on a distinguished road
Jordan is spot on.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 11-16-2017, 07:14 PM
Mike McCain
Guest
 
Posts: n/a
That is an option Paragon offers... At several hundred dollars for the service. I also kinda prefer IFB.
Reply With Quote
  #5  
Old 11-16-2017, 08:15 PM
Eric Trulson Eric Trulson is offline
Young Turk
 
Join Date: Sep 2014
Location: NH
Posts: 70
Eric Trulson is on a distinguished road
Quote:
Originally Posted by Mike McCain View Post
That is an option Paragon offers... At several hundred dollars for the service. I also kinda prefer IFB.
If you want to save money and have a weekend or two to spend working on things, you can build this yourself for comfortably under a grand. Probably more like $500, maybe $600 with hawaii shipping.
Reply With Quote
  #6  
Old 11-17-2017, 01:34 AM
Mike McCain
Guest
 
Posts: n/a
If I were back east, with my tools, I would fabricate my own pick up oven. Out here that's not an option, and I'd just like to know if I can slap something on to the bricks so they won't shed. I'd rather not pay an extra 400$ for the fiber board " upgrade"
What's the stuff used to harden fiber blanket? Thanks
Reply With Quote
  #7  
Old 11-17-2017, 07:07 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 19,829
Pete VanderLaan is on a distinguished road
Colloidal silica, or alumina is the "Stuff" but it isn't going to do what you want. Stuff is falling since th IFB are deteriorating a bit further in than where the coating is going to penetrate.
Further shipping of those products can't happen as a fluid if it has the potential of freezing.

I think replacing it with a mullite kiln shelf is another option but it would take longer to heat up.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 11-17-2017, 02:43 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 532
Charles Friedman is on a distinguished road
Use a thin sheet of SS.
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
  #9  
Old 11-17-2017, 02:48 PM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is online now
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,301
Rich Samuel is on a distinguished road
Charles, this is off topic but, is the DaVinci that just sold the same one that was shown at the Henry in '82?
Reply With Quote
  #10  
Old 11-17-2017, 04:53 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,573
Jordan Kube is on a distinguished road
Best of luck!
__________________
WWUD? Think for yourself.
Reply With Quote
  #11  
Old 11-17-2017, 05:29 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 19,829
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Jordan Kube View Post
Best of luck!
******
Appropriately put.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #12  
Old 11-17-2017, 06:45 PM
Peter Bowles Peter Bowles is offline
Registered User
 
Join Date: Sep 2002
Location: Breadalbane, Tasmania
Posts: 609
Peter Bowles is on a distinguished road
Not wishing to be obtuse, but a clam shell kiln is not the most ideal set up for roll-ups. You'll have to pluck the plates out with gloves to get them onto the fork, can be done of course, but not the most ideal.
If you haven't already got the kiln have a look at getting a front loading kiln, and even better something with the elements in the ceiling.
Reply With Quote
  #13  
Old 11-17-2017, 07:31 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 532
Charles Friedman is on a distinguished road
I have used a clamshell oven to do small roll ups. It has a SS liner above the glass that is ready to be rolled up.

I have a larger oven that is IFB, with the heater elements inside of quartz tubes, that are above the glass. Forks are Easley used to pull out, if needed.

PS Rich yes. http://www.artguidenw.com/LeoEd.htm
__________________
"Glass will save the world from ourselfs" CharlesF

Last edited by Charles Friedman; 11-17-2017 at 07:38 PM.
Reply With Quote
  #14  
Old 11-17-2017, 08:08 PM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is online now
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,301
Rich Samuel is on a distinguished road
Charles, I thought so, too, but then I saw this. The one at the bottom has the provenance I recall and looks a lot more familiar. Looks like Leonardo couldn't decide if he liked his Jesus cross-eyed or wall-eyed.

https://www.italian-renaissance-art....tor-Mundi.html
Reply With Quote
  #15  
Old 11-17-2017, 08:36 PM
Cecil McKenzie Cecil McKenzie is offline
Registered User
 
Join Date: Feb 2011
Location: Emporia, KS
Posts: 461
Cecil McKenzie is on a distinguished road
Colloidal Silica and powdered zircon are the ingredients of z wash. The zircon does not dissolve so you need to stir it. It may be easier to put on if you turn oven over so roof is flat . Good stuff ... May or not solve your problem, Ceramic shops often carry zircon as an opacifier or to make glazes white. Metal casting shops carry colloidal silica and may sell you a little. I think I would try to get a serous wash on at one time rather than several coats. I have noticed a few times it not wanting to stick to itself.
Reply With Quote
  #16  
Old 11-17-2017, 09:27 PM
Marc Carmen Marc Carmen is offline
Registered User
 
Join Date: Jul 2015
Location: New Jersey
Posts: 76
Marc Carmen is on a distinguished road
I've had terrible issues with the 16" paragon clamshell (the one with two handles that opes two ways). If you need reasons not to buy it I'd be happy to elaborate. The clamshells that only open one way are probably much less problematic.

Simply put, brick just doesn't belong in a clamshell. I've since replaced the bricks with fiberboard and am pretty happy with it. Also, blowing out the element channels with compressed air before you heat up helps a lot with brick dust.
Reply With Quote
  #17  
Old 11-18-2017, 12:50 AM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,573
Jordan Kube is on a distinguished road
Quote:
Originally Posted by Marc Carmen View Post
Also, blowing out the element channels with compressed air before you heat up helps a lot with brick dust.
I would start with a vacuum with good suction before you go blowing brick dust all over your studio. Wouldn't hurt to vacuum the whole thing.
__________________
WWUD? Think for yourself.
Reply With Quote
  #18  
Old 11-18-2017, 08:40 AM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 533
Josh Bernbaum is on a distinguished road
Mike, if you're dead-set on using the kiln with IFB's, my idea would be to cut-to-fit a sheet of 1" white fiber board and secure with drywall screws (or SS if you're going higher-temps in there) into the soft brick ceiling. Then you could proceed with sealing your ceiling (I love that) with the colloidal alumina.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #19  
Old 11-18-2017, 10:36 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,163
Eben Horton is on a distinguished road
Id use 2 layers of 2" fiber blanket supported to the ceiling with stainless washers and bolts. then Id hang the elements inside quartz tubes. You could make this conversion in a few hours.
Reply With Quote
  #20  
Old 11-18-2017, 12:54 PM
Mike McCain
Guest
 
Posts: n/a
Thanks for the advice. Any product reviews are welcome. It's a lot of money for me, and I can't justify paying $400 for a 14" square of fiberboard "upgrade."
I suppose when the time comes and the bricks are depleted, I'll do the swap out myself.
Reply With Quote
  #21  
Old 11-19-2017, 11:15 AM
Nick Delmatto Nick Delmatto is offline
Registered User
 
Join Date: Feb 2010
Location: Logan, OH
Posts: 34
Nick Delmatto is on a distinguished road
I've had small IFB glory holes that I've coated with AZS 621 mortar. It worked pretty well. If a small chunk breaks off, recoat the exposed surface.
Reply With Quote
  #22  
Old 11-19-2017, 10:06 PM
Mike McCain
Guest
 
Posts: n/a
Thank you Nick.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 02:27 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.