Blowers

Kevin Ragaller (Rags) used Buffalo forge blowers, 1 ea. For his furnace and 1 for his GH.
VERY quiet, . and operated with Gibby Burners .
Could barely hear them
Jim Antonius
+1 on Jordans info
Reply With Quote
  #27  
Old 12-09-2017, 06:52 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 19,448
Pete VanderLaan is on a distinguished road
It doesn't seem clear that they are still making things Jim. Is that info I don't have?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #28  
Old 12-09-2017, 08:20 PM
Jim Antonius's Avatar
Jim Antonius Jim Antonius is offline
Registered User
 
Join Date: Jun 2002
Location: Prescott, Arizona
Posts: 49
Jim Antonius is on a distinguished road
U can typically find them in Antique Stores, some foundry suppliers and Independent Blacksmiths
Rags operated his with common washing machine motors. It was quiet and he had to choke it down with a flap over the intake.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 08:47 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.