Air-trap twist with three bubbles

Hey gang,

I'm forwarding a question for a friend, Randi Solin, who is another glass blower some of you probably know. She was asked to do a commission to reproduce a (now deceased) glass blower's design to match some of his former pieces when he was still around. Randi is on the fence about the ethics of that for now..
She asked me for recommendations on technique about how to get this trio of bubbles of different colors to twist in solid glass. I'm familiar with the tech for the air twist old English goblet stems, but this has color(s) and the scale is 6" tall by 3" wide. I'm stumped on how to attempt this without trapping unwanted air in the mix. I'm including a photo. Thoughts/suggestions?
Attached Images
File Type: jpg Helix Cylinder 042903.jpg (43.0 KB, 109 views)
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #2  
Old 09-24-2018, 02:22 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,486
Eben Horton is on a distinguished road
Snip 3 colored bits on the bottom of a gather and with a stainless rod, or 3 stainless rods, push the color up into the gather. Then gather over it and twist.

Was this Paul Harries work? If so with the blessing of his wife, I took over the last commission he was working on before he died. I looked at it as an honor.
__________________
<eben epoiese>
Reply With Quote
  #3  
Old 09-24-2018, 02:27 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,024
Pete VanderLaan is on a distinguished road
I miss Paul. A fine designer and a really nice person.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 09-24-2018, 02:34 PM
Josh Bernbaum Josh Bernbaum is online now
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 604
Josh Bernbaum is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
Snip 3 colored bits on the bottom of a gather and with a stainless rod, or 3 stainless rods, push the color up into the gather. Then gather over it and twist.

Was this Paul Harries work? If so with the blessing of his wife, I took over the last commission he was working on before he died. I looked at it as an honor.
Thanks Eben. I thought about that but was imagining that one would loose too much of the fresh furnace heat for pushing in the stainless rods after one has to take the time to snip those bits of color off. But perhaps I'm not thinking about moving quickly enough.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #5  
Old 09-24-2018, 02:53 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,486
Eben Horton is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
I miss Paul. A fine designer and a really nice person.
I never really knew him but did admire his work.
__________________
<eben epoiese>
Reply With Quote
  #6  
Old 09-24-2018, 02:59 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,486
Eben Horton is on a distinguished road
Quote:
Originally Posted by Josh Bernbaum View Post
Thanks Eben. I thought about that but was imagining that one would loose too much of the fresh furnace heat for pushing in the stainless rods after one has to take the time to snip those bits of color off. But perhaps I'm not thinking about moving quickly enough.
Yeah. Do it all quick. Never let your post stop moving. And I would also recommend doing a massive one the size of a 18 block and pulling it into a basebal bat length to anneal. Then diamond saw pieces out of it that you can close the end while you twist, and then take a final gather over it. I believe Paul made a lot of his work like this. You could also pick up 3 pieces of color bar at once off of a plate instead of doing it as a hot bit.
__________________
<eben epoiese>
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:10 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.