Weird melt results..

Sorry, didn't know how to properly title this thread, but I'm super confused..
I've done lots of melts over the years and I haven't seen results like this last one I melted a few days ago. I've been doing phosphate melts lately, 5 total, all mixing in with the SP Plain batch (no erbium). And I know, calcium etc, but I have been getting decent results for the most part. I'd been struggling with the fit but on that 5th melt I finally got it to fit the SP w/er clear I melt also.

Fast forward to my most recent melt this week, where I just wanted a transparent copper blue. I scooped out as much as possible from the bottom of the pot before charging this mix that was the SP plain with 0.77% black copper oxide. It's a gas furnace, my crown is in good shape and my melt times and temps were similar to what I've always done for melts like this.

I've done many, many ionic colors this way over the years but this melt was full of 'snot' that looked like semi see-through white-ish clumps. All throughout the 80 lb pot. My first thought was that, even though I'd scooped out the previous phosphate melt as best I could, that whatever residue from that was making snot in this melt. BUT, what's even weirder, is that compatibility was off, something I don't think I've ever seen with less than 1% addition of colorants to a transparent base. The ring cup I made didn't fare well on the saw, and the only info I could glean from it was that expansion of this blue might be low. My next thought then, is could I have gotten an 'off' bag of SP plain? Unlikely I'd think, as in my experience SP have been so consistent which is one of the many reasons I've stuck with their batch over the years.

Not sure what to do next but I've 'swabbed' the walls of the color pot today with some clear from my main furnace, scooped that out of the bottom, and I'm charging maybe a third of a pot of plain batch next for a 'rinse' that I'll scoop out to try and fully clean this thing. Am I missing something else I should be considering? Thanks in adv, and hope everyone had a good Fourth.

Best,
Josh B
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 06:49 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.