The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,276
Pete VanderLaan is on a distinguished road
If you can gather the glass to make the foot directly on to the stem, you can do an awful lot. It takes about four hours to learn to use a footing tool and to make the gather well.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #27  
Old 10-21-2020, 06:38 PM
phil taylor phil taylor is offline
Registered User
 
Join Date: Sep 2016
Location: cincinnati, ohio
Posts: 7
phil taylor is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
If you can gather the glass to make the foot directly on to the stem, you can do an awful lot. It takes about four hours to learn to use a footing tool and to make the gather well.
As a potter also i loved being taught to do that and also using wet paper to make a foot.
Reply With Quote
  #28  
Old 10-21-2020, 06:52 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,776
Eben Horton is on a distinguished road
Who remembers Brioni ?? He would buy cases of factory made wine glasses and would cut the stems off, and epoxy the tops onto stems he made. He was like the Ron Jeremy of wholesale craft shows.
__________________
<eben epoiese>
Reply With Quote
  #29  
Old 10-21-2020, 07:48 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,276
Pete VanderLaan is on a distinguished road
Did you know he's ( was) Steve Fellerman's first cousin?

He was a Trump style marketer. I remember his speech at the Rosen when he proposed the entire glass group give itself an award. He actually really knew his fraudulent shit well. Stems from Pier One and he made the cups and glued them on.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #30  
Old 10-21-2020, 10:18 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,776
Eben Horton is on a distinguished road
No way! No I didn’t know that they were cousins. Too funny.
__________________
<eben epoiese>
Reply With Quote
  #31  
Old 11-19-2020, 05:26 PM
Paul Thompson Paul Thompson is offline
Registered User
 
Join Date: Apr 2007
Location: Silver Spring MD
Posts: 201
Paul Thompson is on a distinguished road
Quote:
Originally Posted by Shawn Everette View Post
The last time I was on the pad about 12 years ago, I was probably 2 sheets to the wind doing a end of session solo challenge making a cowboy hat with only a modified copper pipe for a tool. I can't say as I remember seeing a pipe hanger, but it sure would have come in handy. Can't say as I remember much about the rest of the night either, and I might be better off for it.
How'd that chapeau turn out for ya, buckaroo?
__________________
"You don't have to be a very good glassblower when you can fix stuff" -- Richard Royal
Reply With Quote
  #32  
Old 11-20-2020, 08:34 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 696
Shawn Everette is on a distinguished road
Much better than I would have thought, actually.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 06:50 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.