potash base glass

I have been reading a lot about how potassium rich glasses typically show brighter colors. So I am interested in creating a potash base glass for some colors. Could anyone give me some general percentages for me to get started with? much appreciated.
Reply With Quote
  #2  
Old 07-24-2017, 05:08 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,306
Pete VanderLaan is on a distinguished road
Maintain your normal max alkaline flux at 18 %. Make about five to six percent of that Potassium Carb or Potassium hydroxide if you don't want all the oxygen. It should be sufficient and will greatly enhance color with selenium, manganese and nickel.
It does increase the viscosity of the glass but at the same time greatly increases the luster. If you can replace calcium with Zinc, you have an excellent base for cadmium selenium reds.
You could likely increase the potassium and cut down on the soda and I would be interested in your color tests as you go up. Potash is expensive stuff compared to sodium so reality beckons to get you to use both. Now if you can get the calcium out completely replaced by barium you will get a profoundly brilliant glass that polishes like a dream and makes copper blues gorgeous. This would not work out that well making the reds. My clear base is a potash barium glass . Jim Myers at East Bay Batch will mix it for you in Oakland. Spruce Pine has indicated that they don't want to stock potassium products which makes it really hard. I won't replace with sodium.

If you haven't stored Potassium carb before, when you get your bag in, immediately take it out and put it in zip lok bags or it will start to take on moisture from the air. Don't store the bags on the ground, get them up on pallets and that's true f most of the forming chemicals. The difference in temp from a cool floor and a warm air, and vice versa make for condensation which really messes up the materials.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 07-25-2017, 05:49 PM
Shawn Watt Shawn Watt is offline
Registered User
 
Join Date: May 2010
Location: Branson, MO
Posts: 101
Shawn Watt is on a distinguished road
Thank you Pete.
Reply With Quote
  #4  
Old 07-30-2017, 03:22 PM
Shawn Watt Shawn Watt is offline
Registered User
 
Join Date: May 2010
Location: Branson, MO
Posts: 101
Shawn Watt is on a distinguished road
so where do you get the potassium hydroxide? All I can really find is the flake form and I imagine that wont mix very well.
Reply With Quote
  #5  
Old 07-30-2017, 07:16 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,306
Pete VanderLaan is on a distinguished road
KOH and it is indeed available as a crystal. To the point where the dealer in Providence insists that potassium carbonate doesn't exist.
I don't think it s critical to have. Dudley was always peculiar in wanting it but you can overwhelm the carbonate with stannous oxide without breaking a sweat. I don't stock it and he keeps trying to sell me his. Any of the potassium compounds are going to be hydrophilic so you have to get them away from humidity. Either use zip locs or air condition the storage shed.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 07:49 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.