Originally Posted by Shawn Everette View Post
The quality of the boro coming from there has really improved over the past 10 years. Doesn't hold a candle to the us color or german clear, but a marked difference from what it once was.
Ive tried a lot of different boro clears and color and Im still not using ANY chinese produced glass. I used chinese produced white for a bit but certainly there is way too much variability for me. I have 4 pounds of it still sitting on my shelf gathering dust. For clear I find Simax to be the best quality and consistency and for me thats critical.
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 08:58 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.