Bomma and Antimony

Noticing that the Bomma does not respond as much to a squeeze as much as the Cristalica and the Spectrum did. Could this be because there is less antimony in it making the valence switch?
Reply With Quote
  #2  
Old 09-01-2020, 08:51 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,310
Pete VanderLaan is on a distinguished road
well, about a gram per lb of antimony is what would normally go into a glass batch. If there isn't sufficient antimony, that could be the issue. Viscosity could have an effect as well.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 09-01-2020, 10:58 AM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,782
Eben Horton is on a distinguished road
Art,
There was a bad batch of Bomma sent over here and it drove a lot of glassblowers nuts because it wouldn’t fine out. I suspect you have some of that batch if you are having troubles
__________________
<eben epoiese>
Reply With Quote
  #4  
Old 09-01-2020, 11:07 AM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 723
Art Freas is on a distinguished road
No serious problems, just seeing different behavior and curious.
Reply With Quote
  #5  
Old 09-01-2020, 12:22 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 696
Shawn Everette is on a distinguished road
You got a production date on that?

I'm about to the end of the stuff I bought June '19 with a March '19 bag date. The stuff I just bought is from May-July '19. Sure doesn't seem like there moving through it that fast.
Reply With Quote
  #6  
Old 09-02-2020, 11:44 AM
Scott Novota's Avatar
Scott Novota Scott Novota is offline
AbbyNormal User
 
Join Date: Jan 2004
Location: Pensacola Florida
Posts: 2,170
Scott Novota is on a distinguished road
I just got some recently and it is the 07/21/2019 run. (shipped from Atlanta)

It fines out just fine for me at 2150f and walking away and doing nothing else. I am just giving it a run to see where it falls compared to SP and how much of a difference it makes in how I work/time. If I was wire this would be what I used. Right now I am on the fence. It does need to work a bit hotter than SP and has, to me at least, a slightly different lockup on the backend. Other than that decent glass.

Furnace: Moly: 2150f load up, put it about 20lbs every 45 min until full. Blow the next morning no issue and never touch the temp. Work it at 2100f. I worked SP at 2050f.

I think I am going to ask for Pete's mix next time and see how I like it. Hell I might even mix my own if I could find a decent silica supplier.


Quote:
Originally Posted by Shawn Everette View Post
You got a production date on that?

I'm about to the end of the stuff I bought June '19 with a March '19 bag date. The stuff I just bought is from May-July '19. Sure doesn't seem like there moving through it that fast.

Last edited by Scott Novota; 09-02-2020 at 11:47 AM.
Reply With Quote
  #7  
Old 09-06-2020, 10:24 AM
Pringle Teetor's Avatar
Pringle Teetor Pringle Teetor is offline
Registered User
 
Join Date: Jul 2003
Location: Chapel Hill, NC
Posts: 662
Pringle Teetor is on a distinguished road
Does anyone have the number on the bad batch? We spent 2 months trying to get the stuff to fine out and gave up.

Quote:
Originally Posted by Eben Horton View Post
Art,
There was a bad batch of Bomma sent over here and it drove a lot of glassblowers nuts because it wouldn’t fine out. I suspect you have some of that batch if you are having troubles
Reply With Quote
  #8  
Old 09-06-2020, 12:33 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,310
Pete VanderLaan is on a distinguished road
Pringle,
You just seem to have the plagues of JOB when it comes to getting bubbles out of things. I had never heard of any bad batch issue with BOMMA but I did find Charlie Parriot in what I would call less than a forthcoming mood whenever I've talked to him about it. Does the cullet have bubbles in it to begin with?

I don't know why it is so seemingly difficult. SP87 made a fine cullet as far as it goes but had the failure of the furnace as an issue. There are commercial furnaces out of South Korea that will handily melt a ton a day without issues for about 50K. The work appears to be ladling it out to turn into the cullet. Now, after two years it seems like the problem has not resolved. You still can't make money on it given the current pricing and that's dangerous.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #9  
Old 09-06-2020, 08:20 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 723
Art Freas is on a distinguished road
Pringle, that is so strange. I will check my bag dates this week. They are from 2019, I think from Oct 19. I did have some seed challenges when we first loaded the pot from cold. Will filled it cold and then brought it up slow, then topped it up. Doing it again I wouldn't load as much at first. would load slower in small layers. We used to load once a week but now we do it a little most nights just keeping it at our working temp of 2150 (with a side thermocouple). After the first load they eventually worked out but it just doesn't respond to a squeeze the same as the cristalica or Spectrum Sys 96.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 12:45 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.