Roll-up technique questions

I have been working on the roll up technique using knobs. Like the ends of pieces that have been pulled off to make what I call a monkey bread plate. This process is particularly interesting to me and I would like to develop it. And so I would like to work with other options to enhance my designs. So my question/s is what types of flat glass (companies) work well with Spruce Pine Batch. What are the different factors to consider when combining a flat glass with SP? Also are there certain colors of rod (Kugler,Reichenbach,, Zimmermann) that do not work well with the flat sheets? I know that is a bad question because of many varibles. I am thinking like particular known color combinations of sheet #'s and bar? What companies sell the flat stuff (sources)?
Also, I am going to experiment with a ceramic kiln shelf/kiln & kiln wash. How do I go about keeping the wash particles off the glass? I ve seen different people use a wicker brush, or some sort of brush?
Art Ciccotti
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On
Forum Jump


All times are GMT -5. The time now is 03:39 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.