CraftWEB Hot Glass Talk  

Go Back   CraftWEB Hot Glass Talk > Hot Glass > Antiques & Classics

Reply
 
Thread Tools Display Modes
  #1  
Old 03-12-2010, 08:35 PM
David Trent David Trent is offline
Registered User
 
Join Date: Dec 2009
Location: Perth Amboy, NJ
Posts: 21
David Trent is on a distinguished road
annealer wiring diagram?

new here.

hoping to get some guidance on the basic components of the wiring of an annealer.

like, I know there are elements on one end, and 220V on the other, and computer controller somewhere in the middle, but what are all the relays and ohter parts, where do they go...how does it all fit together?

is there a drawing or diagram out there that shows this?

thank you.
Reply With Quote
  #2  
Old 03-13-2010, 08:32 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,293
Pete VanderLaan is on a distinguished road
Pg 242 of the 4th edition of Glassnotes shows an interesting drawing of a simple wiring diamgram Fritz did about forty years ago, but it's not very good.

Think of it like this:
Power comes in in two hot legs that go into a switching mechanism called a relay. You put the two hot leads on one side of the relay and then the outbound power on the other side which gets hooked to both ends of your 240V element. The relay is controlled by a solenoid if it's mechanical. Mercury relays last longer than mechanicals but are getting harder to legally use. When power is applied to the solenoid on the relay, the circuit closes and power flows to the element you have. When power is withdrawn, the circuit opens and power to the element shuts off. The controller has a thermocouple input on it which measures milliamps from the thermocouple. Your controller has adjustable settings on it which when the milliamps are matched with the thermocouple, power goes from the controller to the solenoid on the relay. When the controller to the gets turned on, or off,that in turn powers or shuts off the element.

It's just a big assed light switch with some bells and whistles. That's actually true of a moly furnace as well. It just has a rectifier in line which breaks the sine wave up into manageable bite size chunks.

If you can, just go and look in someone's control panel and follow the wires. It's not hard if you are remotely mechanically inclined.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 03-14-2010, 09:53 AM
David Trent David Trent is offline
Registered User
 
Join Date: Dec 2009
Location: Perth Amboy, NJ
Posts: 21
David Trent is on a distinguished road
Thank you for the detailed response Mr. VanderLaan. I do not have a copy of that book at the moment, but I just ordered it online. you mention that the diagram is not very good, im hoping somebody here has a simple one or could draw one that is usable and post it. thanks again.
Reply With Quote
  #4  
Old 03-14-2010, 10:49 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,293
Pete VanderLaan is on a distinguished road
You are way too polite to survive in cyberspace David. I don't have the patience to draw stuff and then make prints of it in computerland. I am sure some deft soul will jump in here. Any simple electricity made easy book would show a diamgram of the principals I'm talking about. Follow the written word.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 03-14-2010, 12:36 PM
Dennis Hetland Dennis Hetland is offline
Registered User
 
Join Date: Sep 2009
Location: Salem, OR
Posts: 304
Dennis Hetland is an unknown quantity at this point
This link will tell you way more about control circuits than you ever wanted to know. http://www.thelearningpit.comhttp://www.thelearningpit.com
Reply With Quote
  #6  
Old 03-14-2010, 03:23 PM
Ben Solwitz Ben Solwitz is offline
Registered User
 
Join Date: May 2008
Location: Brooklyn, NY
Posts: 591
Ben Solwitz is on a distinguished road
Check out the Digitry GB1 manual, it has a bunch of diagrams, starting around page 33:
http://www.digitry.com/pdfs/gb1aman.pdf
The Watlow 982 manual has more technical diagrams, if that's what you're looking for:
http://www.watlow.com/literature/pro...2001-12-07.pdf

Last edited by Ben Solwitz; 03-14-2010 at 03:31 PM.
Reply With Quote
  #7  
Old 03-14-2010, 06:44 PM
David Trent David Trent is offline
Registered User
 
Join Date: Dec 2009
Location: Perth Amboy, NJ
Posts: 21
David Trent is on a distinguished road
thank you, Ben. the GB1 document link you sent has the exact type of diagrams I'm looking for, several good ones actually. what is a good source for the parts needed to re-wire an annealer like the relays, controllers, etc.?
Reply With Quote
  #8  
Old 03-14-2010, 07:26 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,293
Pete VanderLaan is on a distinguished road
DuraLite in Riverton Ct 888-432-8797 will make you elements to order and is the single best source of them I know of.

Controllers
***********
Dwyer (Love) controllers is one supplier www.love-control.com
Fuji www.fujielectric.com
Digitry www.digitry.com

Relays
*************8
Continental Industries int
www.cicontrols.com/contact

Payne Engineering
www.payneng.com

As well as Graingers and McMaster Carr

The book you have bought from Henry Halem "Glassnotes" will have extensive sources of suppliers in the back.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #9  
Old 03-17-2010, 04:15 PM
Dennis Hetland Dennis Hetland is offline
Registered User
 
Join Date: Sep 2009
Location: Salem, OR
Posts: 304
Dennis Hetland is an unknown quantity at this point
lead wires

What type of wire goes from my terminal block to the pig tails of my wire elements? Is it type PFAH or TFE? I'm sure it must be nickel or nickel alloy, but what type is it and where is the best place to buy it?
Reply With Quote
  #10  
Old 03-17-2010, 04:23 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,717
Jordan Kube is on a distinguished road
842° F Braided Wire

Great for internal wiring of an oven, this
flexible single-conductor wire withstands
temperatures up to 842° F. Also called lead wire and Type MG wire,
it has a stranded nickel-plated annealed copper conductor with an
insulation of glass-reinforced mica tape covered with a braided fiberglass
jacket. Temperature range is –40° to +842° F. Color is tan. UL
recognized and CSA certified. Maximum continuous length is 100 ft.

I use this stuff from Mcmaster Carr in a pinch.
__________________
WWUD? Think for yourself.
Reply With Quote
  #11  
Old 03-17-2010, 10:09 PM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 680
Lawrence Duckworth is on a distinguished road
Quote:
Originally Posted by David Trent View Post
new here.

hoping to get some guidance on the basic components of the wiring of an annealer.

like, I know there are elements on one end, and 220V on the other, and computer controller somewhere in the middle, but what are all the relays and ohter parts, where do they go...how does it all fit together?

is there a drawing or diagram out there that shows this?

thank you.
I’m new too, is there any chance you might post photos of the build?

Last edited by Lawrence Duckworth; 03-19-2010 at 01:12 PM. Reason: url link is broken
Reply With Quote
  #12  
Old 03-18-2010, 12:06 AM
Dennis Hetland Dennis Hetland is offline
Registered User
 
Join Date: Sep 2009
Location: Salem, OR
Posts: 304
Dennis Hetland is an unknown quantity at this point
Thanks Jordan.


That's some nice looking equipment Lawrence.
Reply With Quote
  #13  
Old 03-18-2010, 08:05 AM
Rick Sherbert's Avatar
Rick Sherbert Rick Sherbert is offline
Registered User
 
Join Date: Jul 2002
Location: Washington D.C. area
Posts: 728
Rick Sherbert is on a distinguished road
Quote:
Originally Posted by David Trent View Post

Mr. VanderLaan..
.........
Reply With Quote
  #14  
Old 03-28-2010, 12:52 PM
David Trent David Trent is offline
Registered User
 
Join Date: Dec 2009
Location: Perth Amboy, NJ
Posts: 21
David Trent is on a distinguished road
what are "SSR"s and "SCR"s, and where do they fit into the equation?
Reply With Quote
  #15  
Old 03-28-2010, 01:09 PM
Ben Solwitz Ben Solwitz is offline
Registered User
 
Join Date: May 2008
Location: Brooklyn, NY
Posts: 591
Ben Solwitz is on a distinguished road
Solid State Relays are electronic switches, like a mercury relay, but all electronic. Silicon Controlled Rectifiers are solid state devices for controlling current, they limit the power going to resistive heating elements like those used in moly or kanthal a1 furnaces or annealers. Most people don't use them for a1 elements but you can get better element life because you can run the elements continuously at 50% or 60% or whatever instead of switching them between 0% and 100%.
Reply With Quote
  #16  
Old 03-28-2010, 01:26 PM
David Trent David Trent is offline
Registered User
 
Join Date: Dec 2009
Location: Perth Amboy, NJ
Posts: 21
David Trent is on a distinguished road
i think this is the best diagram I've seen so far. Neither the halem nor the giberson books have a wiring diagram, which is surprising. this diagram is for a furnace not an annealer but the general principal i think is the same. a couple things about this diagram confuses me:

what is the plug for? i get that the 110v receptacle powers the temp controller and the 220v receptacle powers the elements but i don't get the whole plug thing on the bottom left. (or, the 220v plug powers the elemts and i don't get the whole 220 receptacle on the bottom right)
Attached Files
File Type: pdf Fuji Control Box.pdf (20.5 KB, 84 views)
Reply With Quote
  #17  
Old 03-28-2010, 01:50 PM
Ben Solwitz Ben Solwitz is offline
Registered User
 
Join Date: May 2008
Location: Brooklyn, NY
Posts: 591
Ben Solwitz is on a distinguished road
It looks like the 220v plug on the left is powering the whole system and the system is providing 110v and 220v receptacles on the right.
Reply With Quote
  #18  
Old 03-28-2010, 02:17 PM
Dave Hilty's Avatar
Dave Hilty Dave Hilty is offline
Registered User
 
Join Date: Apr 2002
Location: Oxford, MI
Posts: 632
Dave Hilty is on a distinguished road
This is essentially the way mine is wired. Ben is right. The plug is the power supply to the entire circuit feeding 110v to the Fuji, the relay that breaks power to the elements when the door is opened and the 110 V receptacle. Don't know what you might need that receptacle for but the easy answer on the 220 V. receptacle is it's an easy way to pick up power from the control circuit to be fed to the elements. Off the shelf hardware store dryer plug & wire package is what I used to feed the anealler elements. It's convenient to use a compatible 220 v receptacle mounted in the control box to plug in the elements.
__________________
Dave Hilty
Reply With Quote
  #19  
Old 03-28-2010, 03:41 PM
David Trent David Trent is offline
Registered User
 
Join Date: Dec 2009
Location: Perth Amboy, NJ
Posts: 21
David Trent is on a distinguished road
Quote:
Originally Posted by Dave Hilty View Post
This is essentially the way mine is wired. Ben is right. The plug is the power supply to the entire circuit feeding 110v to the Fuji, the relay that breaks power to the elements when the door is opened and the 110 V receptacle. Don't know what you might need that receptacle for but the easy answer on the 220 V. receptacle is it's an easy way to pick up power from the control circuit to be fed to the elements. Off the shelf hardware store dryer plug & wire package is what I used to feed the anealler elements. It's convenient to use a compatible 220 v receptacle mounted in the control box to plug in the elements.
i think i got it. please tell me if i am mistaken:
i orignally thought the 110v receptacle was used to plug in the adapter for the fuji, but the plug/adapter was not being shown in the daigram. i think i realize now this is not the case. we are not sure why the 100v receptacle is being used.

so the entire system is powered by the 220v plug in the bottom left. the fuji is running off just the L1 leg of that 220v, which is only 110v since its just one leg.

since the fuji doesn't draw much, L1 can still be used to power an element, which is "the top one" in the drawing.

L2 powers the bottom element

the 220v receptacle is just a cheap way to close the circuits on the other end..
Reply With Quote
  #20  
Old 03-28-2010, 07:01 PM
Dave Hilty's Avatar
Dave Hilty Dave Hilty is offline
Registered User
 
Join Date: Apr 2002
Location: Oxford, MI
Posts: 632
Dave Hilty is on a distinguished road
If you really are feeding two separate elements rather than one as I have, then you need to wire the ends of the elements in parallel to L1 & L2. ie. L1 feeds end A of elements one & two while L2 closes the resistive loop as it is attached to ends B of both elements.
__________________
Dave Hilty
Reply With Quote
  #21  
Old 03-28-2010, 07:39 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,293
Pete VanderLaan is on a distinguished road
Pg 242 of Glassnotes. It's fritz's drawing from 1970 . Get a magnifying glass. It's a terrible drawing.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #22  
Old 03-28-2010, 09:20 PM
Eric Miller's Avatar
Eric Miller Eric Miller is offline
Registered User
 
Join Date: Apr 2009
Location: Columbus, OH
Posts: 203
Eric Miller is on a distinguished road
David-

The diagram that you seek can be found at the beginning of Disk 2 of Mark Lauckner's 40 lb wire melter videos. He actually draws the diagram on a big piece of butcher paper, explains it, lays out the components on the paper, and then spends 30m or so of video explaining how to wire it all together.

In fact, the .pdf you posted is from somebody's (Drew Fritts?) variation of Mark's 15 lb wire melter, which he doesn't sell videos for anymore.

Everything will be the same for your annealer wiring except the way you program the controller and the elements you use.

Get Mark's videos and all your questions will be answered, they are $45. I would have paid twice that for them.

Hope this helps.
Reply With Quote
  #23  
Old 03-28-2010, 11:55 PM
Rick Wilton Rick Wilton is offline
Registered User
 
Join Date: Oct 2005
Location: Calgary, Alberta Canada
Posts: 224
Rick Wilton is on a distinguished road
in that drawing why is there a SSR AND a mercury relay. The SSR appear to only be used to turn the MDR on and off. Why not loose the MDR ( they are illegal now anyway in many places) and just run two SSR. That's how I wired my stuff.
Reply With Quote
  #24  
Old 03-29-2010, 08:52 AM
Dave Hilty's Avatar
Dave Hilty Dave Hilty is offline
Registered User
 
Join Date: Apr 2002
Location: Oxford, MI
Posts: 632
Dave Hilty is on a distinguished road
The ssr controls the 220 feed to the elements via the 220 v. receptacle. The MDR isn't controlled by the ssr, it breaks the circuits so no voltage flows to the elements when the door is open. (see the microswitch actuated by a dog or whatever on the door of the annealer). SSR's leak voltage even when open so they don't provide the complete break in voltage that a mechanical or mercury relay will.
__________________
Dave Hilty
Reply With Quote
  #25  
Old 03-29-2010, 11:06 AM
Rick Wilton Rick Wilton is offline
Registered User
 
Join Date: Oct 2005
Location: Calgary, Alberta Canada
Posts: 224
Rick Wilton is on a distinguished road
DAve,

Got ya, then why is the SSR on a 10 amp.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On
Forum Jump


All times are GMT -5. The time now is 05:54 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.