Quote:
Originally Posted by Dan Vanantwerp View Post
10 lbs. My color crucibles are 17 lbs. I am able to get 6-8 lbs charged before my first blow session Saturday and then top off with the rest for Sunday.
*********
If you are using 10 lb mixes, if I understand that correctly, and you are adding around 300 grams of material to a mix you say Jim at East bay has already mixed, and you suggest it is mostly mixed by east bay, I think you're wrong. What I do think is that you're adding about 8% new materials to Jim's stuff in various semi hostile forms. In my mind, that''s a very large number. so, again, how are you mixing this new stuff in? What is your mixer?

Process is key in doing this stuff.
__________________
Where are we going and why am I in this basket?
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 06:26 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.