adding gold to batch

Hello All,

I was doing some research for my art history class at Alfred University and I came across a cage cup known as the Lycurgus Cup. The green photo is when the cup is lit from the front and the red photo is back lit. I was reading about the composition and it has about .0005% gold as well as silver and manganese. I'm wondering how one adds gold to glass batch. I know you have to dissolve the gold in aqua regia (very nasty). From there, historically, tin has been added to make Purple of Cassius which I believe is a powder. However, on Instagram, I saw a post where someone poured a solution, I don't know if this was the aqua regia with auric chloride or something else like a gold solution with some thing else added, straight onto the batch which was then mixed and other oxides added.

I'm really interested in this because this is a glass that becomes completely different based on how its viewed. There's a duality to the glass, similar to rare earth glasses that change color or uv reactive glasses like uranium.
Attached Images
File Type: jpg download.jpg (11.1 KB, 71 views)
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 08:37 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.