Optic mold trade

Would anyone have a 18-16A mold they would be interested in trading for a
18-8A mold? I would be willing to pay for shipping both ways.
I also have a surplus of molds and tools I would trade for a 18-16A. Iím in need of this mold ASAP so this would have to be a quick turnaround.
Thanks for the consideration.
Reply With Quote
  #2  
Old 08-09-2020, 01:23 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 1,017
Larry Cazes is on a distinguished road
Quote:
Originally Posted by Sky Campbell View Post
Would anyone have a 18-16A mold they would be interested in trading for a
18-8A mold? I would be willing to pay for shipping both ways.
I also have a surplus of molds and tools I would trade for a 18-16A. Iím in need of this mold ASAP so this would have to be a quick turnaround.
Thanks for the consideration.
Steinert, CD?
Reply With Quote
  #3  
Old 08-09-2020, 01:41 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is online now
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 1,019
Sky Campbell is on a distinguished road
I donít know anyone that makes molds this size except Steinert. If you have a 18Ē tall mold with 16 v ribs I would consider any maker.
Reply With Quote
  #4  
Old 08-09-2020, 02:07 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,748
Eben Horton is on a distinguished road
Quote:
Originally Posted by Sky Campbell View Post
I donít know anyone that makes molds this size except Steinert. If you have a 18Ē tall mold with 16 v ribs I would consider any maker.
Is that the largest one they make that is straight sided and open at the bottom?
__________________
<eben epoiese>
Reply With Quote
  #5  
Old 08-09-2020, 09:01 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is online now
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 1,019
Sky Campbell is on a distinguished road
No it’s the largest one and has tapered sides. I had one that I loved but I don’t think it’s coming back. The 8 rib same size mold is a beautiful mold to work larger platters out of but for this job I need it to flow with the existing work I made earlier. I’m not even sure if John has them in stock but sure would love to make a trade then to buy another one.

I just looked and the only two molds of this size are the one I’m trading and the one I’m looking for.

Last edited by Sky Campbell; 08-09-2020 at 09:05 PM.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:42 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.