Mystery Blue Punty Additive

Does anyone know what the stuff is that Janusz Pozniak is adding to his punty is this video of he and Dante making a low bowl? I've attached a screenshot.

Here is the video: https://www.youtube.com/watch?v=0WGgCUVnoQs

Thanks...

P.S. If someone says "glass" just remember that karma is a b#%ch.
Attached Images
File Type: jpg low bowl.jpg (26.2 KB, 81 views)
__________________
My furnace setting: 2112
Reply With Quote
  #2  
Old 08-29-2017, 08:52 PM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,392
Rich Samuel is on a distinguished road
Powdered chalk?
Reply With Quote
  #3  
Old 08-29-2017, 09:10 PM
Dan Vanantwerp Dan Vanantwerp is offline
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 246
Dan Vanantwerp is on a distinguished road
He adds it to the business end as well...would chalk allow for an easy release?
The bowl is a transparent roll-up so a punty mark would be a definite no-no.
__________________
My furnace setting: 2112
Reply With Quote
  #4  
Old 08-30-2017, 12:50 AM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 887
Sky Campbell is on a distinguished road
It very well could be chalk. I've used chalk on the bottom of a vessel to find center and lost pieces for lack of sicktivity. Ok maybe not a scrabble word. Anyway it could be some straight line for a chalk box.

Sand punties have been around forever and I've seen where someone will roll on a piece of ifb before applying. Blue chalk would be my vote.
Reply With Quote
  #5  
Old 08-30-2017, 04:55 AM
Peter Bowles Peter Bowles is online now
Registered User
 
Join Date: Sep 2002
Location: Breadalbane, Tasmania
Posts: 626
Peter Bowles is on a distinguished road
That has to be one of the shittyist demonstrations I've ever seen. Very saddening to see that as the benchmark for students now coming into glass.
So very sad.
Reply With Quote
  #6  
Old 08-30-2017, 07:55 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,504
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Peter Bowles View Post
That has to be one of the shittyist demonstrations I've ever seen. Very saddening to see that as the benchmark for students now coming into glass.
So very sad.
********
Jeez Peter, With just a little work you could turn that into a tweet.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 08-30-2017, 08:39 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,378
Eben Horton is on a distinguished road
chalk. you can also use IFB dust
Reply With Quote
  #8  
Old 08-30-2017, 01:44 PM
Dan Vanantwerp Dan Vanantwerp is offline
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 246
Dan Vanantwerp is on a distinguished road
I'd really like to have Peter elaborate on why the demonstration is so bad? I'm using Dante's sequencing as a learning tool to make better bowl shapes. The final shape looks very good to me. They are very stoic and there is not any great display of teamwork but I'm a solo glassblower and appreciate any video I can find with less than 3 assistants.
__________________
My furnace setting: 2112
Reply With Quote
  #9  
Old 08-30-2017, 04:38 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,378
Eben Horton is on a distinguished road
Quote:
Originally Posted by Dan Vanantwerp View Post
I'd really like to have Peter elaborate on why the demonstration is so bad? I'm using Dante's sequencing as a learning tool to make better bowl shapes. The final shape looks very good to me. They are very stoic and there is not any great display of teamwork but I'm a solo glassblower and appreciate any video I can find with less than 3 assistants.
the secret to a good low bowl is to punty it up with the bowl as hot as you dare and the punty as cold as you dare. Use a big round shaped punty with chalk dust around the edges so it won't fully stick but add support. You can make a bowl with just a newspaper by spinning the half opened bowl fast and "catching" the bowl in your paper to shape it to the final shape
Reply With Quote
  #10  
Old 08-30-2017, 05:39 PM
Dan Vanantwerp Dan Vanantwerp is offline
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 246
Dan Vanantwerp is on a distinguished road
Cool...got to try it out!

I find that a fine line exists with papering a bowl and leaving the dreaded scum...it's all about the heat, but sometimes I just get caught up in trying to perfect the shape.

I like Dante's use of the parchoffis to push out the bottom and sides to widen the shape. His little floor steam puffer step is also pretty nifty.

Randy Walker had a class highly recommended to me: the 1/2 round bowl. Anyone know if he is still teaching?
__________________
My furnace setting: 2112
Reply With Quote
  #11  
Old 08-30-2017, 07:16 PM
Peter Bowles Peter Bowles is online now
Registered User
 
Join Date: Sep 2002
Location: Breadalbane, Tasmania
Posts: 626
Peter Bowles is on a distinguished road
I've had a long love-hate-love thing with bowl making over the years - and to see someone demonstrating with such disdain for the process leaves me cold.
Shitty canes, shitty gather, shitty marvering, shitty blowing, sloppy shearing, aggressive opening. It's just is never going to make a good bowl. He knew it, the team knew it, the students seemed to know it. Just very sad.

If you want to learn bowl making - look to the the Swedes and the Danes. The Scandinavian approach is way more sensitive than anything I've seen out of the Italian tradition.

Everyone who makes bowls have their own thing that they think is critical - sometimes they overlap, sometimes they are in contradiction. It's a fascinating journey. For me, its all about managing wall thickness, when I get that right the bowl helps to make its own lines a lot easier. I used to spend a lot of time chalk drawing on the floor to work through the stages I wanted all the way from gathering through blowing, and opening.

My first off hint would be to lower your yolk 50mm - that in itself will change everything.
Reply With Quote
  #12  
Old 08-30-2017, 07:53 PM
Dan Vanantwerp Dan Vanantwerp is offline
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 246
Dan Vanantwerp is on a distinguished road
Thanks Peter. You certainly have the proper surname to have formed a strong opinion on the subject.

Seriously, though, it's very humbling for me to consider how much time many of you have devoted to your glass in pursuit of the perfect shape.

Any artist(s) in particular I might look to from the Scandinavian school. I believe Buzz Blodgett was trained by his father in this manner. He was teaching an advanced class at UC San Diego while I lived there but I never had the opportunity to attend (and I was no means, advanced). I think their program has now gone defunct.
__________________
My furnace setting: 2112
Reply With Quote
  #13  
Old 08-30-2017, 08:22 PM
Peter Bowles Peter Bowles is online now
Registered User
 
Join Date: Sep 2002
Location: Breadalbane, Tasmania
Posts: 626
Peter Bowles is on a distinguished road
Darryl Hinze, Nanna Bachaus, Tobias Mohl are all great bowl makers, not sure how much is out there on youtube on them. Stephen Dam could also make beautiful bowls, not sure how much of his practice is of that kind now.
Reply With Quote
  #14  
Old 08-31-2017, 12:16 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,633
Jordan Kube is on a distinguished road
I never flash the punty on a low bowl once it's on. It will stay warm from the deep heats.
__________________
WWUD? Think for yourself.
Reply With Quote
  #15  
Old 08-31-2017, 11:45 PM
Dan Vanantwerp Dan Vanantwerp is offline
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 246
Dan Vanantwerp is on a distinguished road
There are some nice videos out there of Nanna. Beautiful studio/gallery with her husband right on a marina. For bowls, her setup and Dante's are very different....interesting contrast in styles. Dante's shape prior to transfer has a fairly long neck and a wide bottom...like an Erlenmeyer flask. He trims off quite a bit to bring the sides down. Nanna spins out the sides while on the pipe in the glory and the shape prior to transfer is much more like the final bowl.

Not sure if this can be generalized but I also noticed how much more she kept the pipe downward. For most of the artists I've watched they tilt the pipe upward with their left hand to look at the piece (I guess) and enter the bench with the right hand ready to grab a tool. Nanna keeps it low and "swings open the gate" to enter the bench. I was taught the gate method but have been trying the other style to get my hands on a tool faster.

Like Jordan suggests, I was taught to NOT flash while working a platter or low bowl. Got to keep it square. Nanna spends a good 2 or 3 turns every time to set the punty end of a bowl. She works QUICK! Out of the glory, to the bench and very efficient. Joy to watch...she is very nice looking also
__________________
My furnace setting: 2112
Reply With Quote
  #16  
Old 09-01-2017, 08:59 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,378
Eben Horton is on a distinguished road
Dream studio!

https://youtu.be/S7QDKfBD9ck
Reply With Quote
  #17  
Old 09-01-2017, 09:19 AM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 577
Josh Bernbaum is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
Wow, nice spot for a shop. I'd like to know what he is sealing that piece with at the end, looks like some heated up wax?
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #18  
Old 09-01-2017, 10:39 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,378
Eben Horton is on a distinguished road
Quote:
Originally Posted by Josh Bernbaum View Post
Wow, nice spot for a shop. I'd like to know what he is sealing that piece with at the end, looks like some heated up wax?
That's what I think as well. Diamond wheel, sand blast off the roughness of the wheel marks and then hot wax.
Reply With Quote
  #19  
Old 09-09-2017, 02:35 PM
Justin Zotynia Justin Zotynia is offline
Registered User
 
Join Date: Aug 2009
Location: Bushkill, PA
Posts: 56
Justin Zotynia is on a distinguished road
there is a great video of boyd and lisa demoing bowls on YouTube at cmog. not enough data to watch Dante
Reply With Quote
  #20  
Old 09-09-2017, 02:41 PM
Justin Zotynia Justin Zotynia is offline
Registered User
 
Join Date: Aug 2009
Location: Bushkill, PA
Posts: 56
Justin Zotynia is on a distinguished road
Studio Demonstrations: Boyd Sugiki & Lisa Zerkowi…: http://youtu.be/k-fEIbNfbWk
Reply With Quote
  #21  
Old 09-13-2017, 08:52 PM
Bradley Howes Bradley Howes is offline
Registered User
 
Join Date: Mar 2015
Location: Palo Alto, CA
Posts: 39
Bradley Howes is on a distinguished road
I agree with the above posts, it does look like chalk.
Reply With Quote
  #22  
Old 09-14-2017, 11:21 PM
Scott Mitchell Scott Mitchell is offline
Registered User
 
Join Date: Jun 2013
Location: Springfield, VA
Posts: 29
Scott Mitchell is on a distinguished road
Ok, what was the point of the extra transfer after the rollup. Why go through closing the bubble, re-opening it, and then transferring to a post?
Reply With Quote
  #23  
Old 09-15-2017, 03:14 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
PotatoFish
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,003
Greg Vriethoff is on a distinguished road
Not long after I landed in Seattle I took a three-day workshop at Pratt in assisting skills. The instructor(s) was one of Lino's main people. When we got to making this kind of punty, it was stressed very heavily that these are called "dust punties." DO NOT refer to them as "sand punties."

Okay.

I asked someone later at the shop I was working at what the deal was. I was told that the term "sand" was associated with what's done down in Mexico.

This stuff gets so stupid at times.
__________________
"It's such a fine line between stupid and clever." - David St. Hubbins

Last edited by Greg Vriethoff; 09-15-2017 at 03:14 PM. Reason: spelling
Reply With Quote
  #24  
Old 09-15-2017, 04:11 PM
Dan Vanantwerp Dan Vanantwerp is offline
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 246
Dan Vanantwerp is on a distinguished road
Thanks to everyone for their contributions and educated guesses. I think that Greg has the winning answer though and even "named" it...dust punty. Kind of sounds like dust bunny...I like it!

Going to grind up some sidewalk chalk and probably lose a few pieces until I figure out the right amount to apply. Then I can use the chalk to outline the remains on the floor.
__________________
My furnace setting: 2112
Reply With Quote
  #25  
Old 09-15-2017, 05:39 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,504
Pete VanderLaan is on a distinguished road
we used to make sand punties. They certainly work unless they don't
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:58 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.