Mesh of silica flour

What mesh silica flour do you use for molds.
I can imagine it linked to the details you want so let's use fingerprints as the highest detail. Will 200 mesh work?
Ok just found I may be able to get 400 mesh.
Franklin

Last edited by Franklin Sankar; 12-10-2017 at 08:38 AM. Reason: More information
Reply With Quote
  #2  
Old 12-10-2017, 08:49 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,698
Franklin Sankar is on a distinguished road
Is flint the same as silica
Franklin
Reply With Quote
  #3  
Old 12-10-2017, 09:05 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,086
Pete VanderLaan is on a distinguished road
325 mesh seems to be the mesh of choice. Flint is silica, is quartz.

I've seen mixes that use both a 200 and a 325 mesh. 325 is considerably more expensive. When I get plaster, I immediately transfer it into airtight canisters that cat food comes in Delicat is my favorite. I must have about 100 or them at this point. If you leave it out in humidity, it will wreck it.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 12-10-2017, 01:53 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,698
Franklin Sankar is on a distinguished road
Thanks. I have been trying to ship this for the longest while.
Franklin
Reply With Quote
  #5  
Old 12-14-2017, 04:44 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,698
Franklin Sankar is on a distinguished road
I got it. The silica not the cat. 400 mesh. It's beautiful.
Franklin
Reply With Quote
  #6  
Old 12-14-2017, 05:04 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,086
Pete VanderLaan is on a distinguished road
The "cat"?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 12-15-2017, 06:19 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,698
Franklin Sankar is on a distinguished road
Just my not so good humor. I follow your footprint exactly as instructed so the need for a cat and the airtight canister. If it don't work it's because I have 3 dogs but no cat.
Franklin
Reply With Quote
  #8  
Old 12-17-2017, 07:02 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,231
Eben Horton is on a distinguished road
How can you make a proper oildown with no Cat?
Reply With Quote
  #9  
Old 12-18-2017, 03:24 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,698
Franklin Sankar is on a distinguished road
Sorry Eben you need Chatine to make that.
Franklin
Reply With Quote
  #10  
Old 12-18-2017, 03:38 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,086
Pete VanderLaan is on a distinguished road
screen your flour, no chat.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:33 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.