cold digitry

My studio got really cold last night and the digitry was reading 32į. I forgot that if it reads that temp, it won't allow the elements to turn on and used a torch on the thermocouple to fool it.

I hope that others don't have this problem and go through a wild goose chase of problem solving.
Reply With Quote
  #2  
Old 01-02-2018, 10:56 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,086
Pete VanderLaan is on a distinguished road
Digitry aside, Colloidal silica and alumina are ruined if frozen. Not to mention the water pipes. We've gone to -29F three nights in a row up here on top of multiple days at -15F or so says accuweather and I'm running a burner in the gloryhole to keep things livable while we rebuild this little furnace. We're going through a lot of firewood.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 01-02-2018, 02:17 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,231
Eben Horton is on a distinguished road
Wow! Thatís cold!! Stay warm Pete!
Reply With Quote
  #4  
Old 01-02-2018, 02:47 PM
Steve Stadelman Steve Stadelman is offline
Registered User
 
Join Date: Jun 2002
Location: Portland oregon area
Posts: 3,734
Steve Stadelman is on a distinguished road
Many controllers use a thermocouple within the instrument case as a reference. I had several installs in cold states that needed a light bulb inside the enclosure to start.
__________________
If all you wanted to do was express yourself artistically, you should have obtained a field watercolor set and a pad of acid-free paper. You chose a media with INFRASTRUCTURE baby!
Reply With Quote
  #5  
Old 01-02-2018, 04:23 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,086
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
Wow! That’s cold!! Stay warm Pete!
**********
The hot water heater still comes from firewood but it's amazing what a 60W light bulb can do in a tent. I mortared yesterday, tented the mess and pushed the furnace over to the glory hole. About 55F in the tent this morning and that's what I needed. Today was more of a horse day and I have to plow out about 1/3 mile to the firewood for a friend who is out, so, that's a day easy. There's 15 cords out there . The truck is showing its age and I don't want a new truck at my age. All this damn salt. I wouldn't mind a second tractor though.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 01-02-2018, 04:37 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,231
Eben Horton is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
**********
The hot water heater still comes from firewood but it's amazing what a 60W light bulb can do in a tent. I mortared yesterday, tented the mess and pushed the furnace over to the glory hole. About 55F in the tent this morning and that's what I needed. Today was more of a horse day and I have to plow out about 1/3 mile to the firewood for a friend who is out, so, that's a day easy. There's 15 cords out there . The truck is showing its age and I don't want a new truck at my age. All this damn salt. I wouldn't mind a second tractor though.
how about a small RV and in november you and your bride hit a warmer climate until spring? Im planning on doing something like this but on a boat.
Reply With Quote
  #7  
Old 01-02-2018, 04:42 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,086
Pete VanderLaan is on a distinguished road
I ain't doing no RV's.
Quote:
"The two best days in owning a boat are the day you buy it and the day you sell it."

But thanks...
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 01-02-2018, 05:40 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,231
Eben Horton is on a distinguished road
I have to disagree with that statement. But maybe Iím an exception as I pretty much grew up on boats.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:33 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.