  #26  
Old 12-08-2017, 07:26 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,739
Jordan Kube is on a distinguished road
Just a quick pull test shows a 2" bend in 16" of stringer, clear inside. It works super stiff in our 2500 degree glory holes too. I'm going to let it sit overnight and play with it tomorrrow.
__________________
WWUD? Think for yourself.
Reply With Quote
  #27  
Old 12-09-2017, 08:55 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,739
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Jordan Kube View Post
Well there's no way this stuff is compatible. Imagine throwing a bunch of zirconia into your melt! The color is beatiful though. I'm probably going to have to melt my own custom clear and offset the expansion if I want to do it this way. I might hit you up for some advice Pete.
*******
Two inches is rather huge. You'll never make a Hagy seal out of it that survives nor will a ring test do anything. I could take a cane 4mm (pencil lead size) diameter and make a run at the dilatometer but I would bet on something in the mid eighties.
This is where it gets hard using cullet, crushed or whatever. It's really hard to add stuff to cullet and remain accurate or not cording it up. If you do try, use potassium or lithium . They'll do different things. Potassium is kind to the color but doesn't move expansion as easily and Lithium will move expansion and make it kind of cordy.
This sort of stuff is likely easier in Boro since it hardly expands in the first place although lithium would wreck it.
Rather than to try to make a clear that's not compatible with the known world, I'd be more inclined to make a conventional assault on the color.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #28  
Old 12-09-2017, 12:37 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,739
Jordan Kube is on a distinguished road
A custom clear with an offset expansion would be the way to go. This doesn't work with batch.

This is after 24 hours in the pot. Again, the pictures don't capture how nice this stuff is. It was the only one I could get out today, the barlett controller decided it didn't want to clear its error message so things are coming down as we speak.
Attached Images
File Type: jpg Red resize.jpg (67.8 KB, 33 views)
__________________
WWUD? Think for yourself.
Reply With Quote
  #29  
Old 12-09-2017, 02:08 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,739
Pete VanderLaan is on a distinguished road
It really looks nice but I suspect a moving target. Keep in mind you can get there with excess amounts of cadmium. That pushes the opacity. I suppose I prefer it when everything is compatible with ever thing else.

Down this path lies madness.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #30  
Old 12-10-2017, 02:49 PM
Kenny Pieper Kenny Pieper is offline
Registered User
 
Join Date: Feb 2003
Location: Burnsville N.C.
Posts: 857
Kenny Pieper is on a distinguished road
Quote:
Originally Posted by Jordan Kube View Post
A custom clear with an offset expansion would be the way to go. This doesn't work with batch.

This is after 24 hours in the pot. Again, the pictures don't capture how nice this stuff is. It was the only one I could get out today, the barlett controller decided it didn't want to clear its error message so things are coming down as we speak.
Is that straight out of the pot , or did you have to strike it? Nice color!
Reply With Quote
  #31  
Old 12-10-2017, 05:39 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,739
Pete VanderLaan is on a distinguished road
Hi Kenny, We haven't talked in a long time. Did you get those selenites I had hoped you could bring from George?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #32  
Old 12-11-2017, 07:10 AM
Kenny Pieper Kenny Pieper is offline
Registered User
 
Join Date: Feb 2003
Location: Burnsville N.C.
Posts: 857
Kenny Pieper is on a distinguished road
Yea Pete I have a number of them I would be happy to share.
Reply With Quote
  #33  
Old 12-11-2017, 07:46 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,739
Pete VanderLaan is on a distinguished road
Thank you. Did the 30 mesh you know what work OK?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #34  
Old 12-11-2017, 01:38 PM
Kenny Pieper Kenny Pieper is offline
Registered User
 
Join Date: Feb 2003
Location: Burnsville N.C.
Posts: 857
Kenny Pieper is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
Thank you. Did the 30 mesh you know what work OK?
Only used it once so far and it was fine. Actually there is a small melt bubbling away in the furnace now with some of the stuff in it. Hopefully a light opal for goblets.
Reply With Quote
  #35  
Old 12-12-2017, 04:32 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,739
Jordan Kube is on a distinguished road
Quote:
Originally Posted by Kenny Pieper View Post
Is that straight out of the pot , or did you have to strike it? Nice color!
Pretty much comes out of the pot like that, Kenny. I'm really excited to work on it but I've got some lower hanging fruit to tackle first.

I'll post up the saw cuts after I make them but might not get to it until next week.
__________________
WWUD? Think for yourself.
Reply With Quote
  #36  
Old 12-12-2017, 11:20 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 1,032
Sky Campbell is on a distinguished road
Quote:
Originally Posted by Scott Novota View Post
This is pretty cool! Where did you get those little assays from? I am interested in doing some stuff myself and those look very handy.
Hey Scott check out this thread for more info:

http://talk.craftweb.com/showthread....nver+fire+clay
Reply With Quote
  #37  
Old 12-13-2017, 11:35 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,739
Pete VanderLaan is on a distinguished road
I'm under the impression that Denver Fire Clay was absorbed by Coors and markets as Coorstek out of Golden. Assay crucibles are certainly a great deal for experiments. They leach a lot of iron making use for clear not good and don't last long but as a throwaway, it's nice.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 07:19 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.