Bomma Bomma Bomma

While we are still trying to fine out this stuff (still no luck), I noticed this on a ball I blew a few weeks ago. Hmmmmm
Attached Images
File Type: jpg 2960F36C-1568-4C13-AE04-31D06D25B754.jpg (54.5 KB, 82 views)
File Type: jpg DDFEA773-AF0B-44BB-8998-31C3F0072DA1.jpg (64.7 KB, 77 views)
File Type: jpg BBD9B2D3-0670-4503-AE9D-650A18D0C695.jpg (37.0 KB, 68 views)
Reply With Quote
  #2  
Old 02-26-2020, 05:59 AM
Pringle Teetor's Avatar
Pringle Teetor Pringle Teetor is offline
Registered User
 
Join Date: Jul 2003
Location: Chapel Hill, NC
Posts: 658
Pringle Teetor is on a distinguished road
This is not a cloudy film on the inside like we had in ornaments with the original spectrum glass. It reminds me of oil slicks on water puddles.
Reply With Quote
  #3  
Old 02-26-2020, 07:43 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,933
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Pringle Teetor View Post
While we are still trying to fine out this stuff (still no luck), I noticed this on a ball I blew a few weeks ago. Hmmmmm
***
It actually looks like really stressed glass under a polarizer. Sometimes you can see that without a filter.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 02-26-2020, 09:00 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 585
Shawn Everette is on a distinguished road
I've had that with things that went into the knock off. Need to figure out how to keep it and sell it as "special reserve".
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 07:12 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.