Thermocouple connector

Anyone use these connectors. I keep getting intermittent failures. I donít think itís the wires since it is so stiff and difficult for it to fail?
The connectorS look fragile.
Franklin
Attached Images
File Type: jpg image.jpg (31.7 KB, 21 views)
Reply With Quote
  #2  
Old 07-18-2020, 08:51 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,120
Pete VanderLaan is on a distinguished road
In the Caribbean, it could be oxidation. Take the thing apart and clean the leads.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 07-18-2020, 09:53 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,041
Franklin Sankar is on a distinguished road
Itís bright and shiny. Looks good. But just in case i will clean.
Franklin
Reply With Quote
  #4  
Old 07-18-2020, 11:44 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,120
Pete VanderLaan is on a distinguished road
I have some of those things that are over thirty years old and they're fine. If it's intermittent, is that with one thermocouple or more than one. If it's one, Look hard at the thermocouple. If it's with more than one, throw away the connector.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 07-18-2020, 05:46 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,041
Franklin Sankar is on a distinguished road
Thanks for confirming it is tried and tested out there. I put a connector between The controler and the thermocouple. It was driving me crazy. Intermittent is the worst. I pulled it out and wired directly and all is well now.
Franklin
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 12:28 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.