Hi George, The positive pressure idea sort of gets to Pete's mention of a reverse blower port to remove the fumes periodically. A continuous system as you describe would seem the better solution. Problem with air turnover is the loss of heat...we might lower the fluorine attack but still decrease the element life by making them work harder.

Although, hot air could be recuperated from a clean source...
__________________
My furnace setting: 2112
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 11:19 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.