Once again: I need 120 mesh SIC grit

Sources? They come and go so fast. I want 120-200 lbs.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #2  
Old 03-30-2018, 08:07 PM
Brian Graham's Avatar
Brian Graham Brian Graham is offline
Registered Abuser
 
Join Date: Mar 2004
Location: Akron - Ohio
Posts: 574
Brian Graham is on a distinguished road
https://www.panadyneabrasives.com/main.sc
__________________
The revolution will not be televised.
Reply With Quote
  #3  
Old 03-31-2018, 02:14 AM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,680
Rich Samuel is on a distinguished road
https://www.washingtonmills.com/prod...ing-polishing/

http://www.kramerindustriesonline.com/SIC.html
Reply With Quote
  #4  
Old 03-31-2018, 11:13 AM
Kenny Pieper Kenny Pieper is offline
Registered User
 
Join Date: Feb 2003
Location: Burnsville N.C.
Posts: 890
Kenny Pieper is on a distinguished road
Its been a while but I use to get it at Salem distributing.
Reply With Quote
  #5  
Old 03-31-2018, 12:27 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 24,091
Pete VanderLaan is on a distinguished road
They do not appear to handle it anymore Kenny and that's true of a number of former jobbers including FUSCO. Two of the three that are listed here were what I thought was really expensive in the 2.00+ lb range with one being a boutique assault at the best over 4.50 lb. I have a quote in for 200 lbs from one supplier not even listed and I'm looking for about $1.20 lb in a single 200 lb drum which is what I used to do only the last time I bought a drum I think it was about a dollar a lb.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 03-31-2018, 03:08 PM
Marty Kremer Marty Kremer is offline
Registered User
 
Join Date: May 2004
Location: North Yarmouth ME
Posts: 580
Marty Kremer is on a distinguished road
I've been using Sunbelt Industries in Little Falls NY for years.
315-823-2943
Reply With Quote
  #7  
Old 04-07-2018, 02:09 AM
neil duman neil duman is offline
Registered User
 
Join Date: May 2015
Location: VA
Posts: 35
neil duman is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
Sources? They come and go so fast. I want 120-200 lbs.
Try JHHorton company in Chesapeake, VA
Reply With Quote
  #8  
Old 04-07-2018, 08:41 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 24,091
Pete VanderLaan is on a distinguished road
Thanks, The recycle from sunbelt is perfect and the price is excellent.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:22 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2023, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.