Jordan,

Strontium will help. Lithium will help a lot.

If you have Volf read up on strontium. Similar effects as lead without the toxicity.

Be very sure you have enough alumina with strontium (Volf) as in sum of 1st column in periodic table divided by eight (Labino).
__________________
Art is not a thing...it's a way.

Last edited by Dave Bross; 02-14-2018 at 06:31 PM.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 02:49 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.