Type of plaster

Is #1 pottery plaster the same as dental plaster? I have no pottery plaster.
Franklin
Reply With Quote
  #2  
Old 07-13-2019, 10:18 PM
Steven O'Day Steven O'Day is offline
Registered User
 
Join Date: Jun 2002
Location: portland oregon
Posts: 322
Steven O'Day is on a distinguished road
No. #1 pottery plaster is straight plaster, dental plaster is a mix of plaster and refractory and maybe other stuff. Each brand has it's own mix so it is difficult to compare them. If you are using this for glass casting you will need to adjust the amount of silica in the mix or maybe just use the dental plaster by itself. The amount of water and mixing technique is important.
Reply With Quote
  #3  
Old 07-13-2019, 10:24 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,956
Franklin Sankar is on a distinguished road
Thanks for the reply. When you say straight plaster do you mean plaster of paris?
I can get dental plaster.
Franklin
Reply With Quote
  #4  
Old 07-13-2019, 10:58 PM
Steven O'Day Steven O'Day is offline
Registered User
 
Join Date: Jun 2002
Location: portland oregon
Posts: 322
Steven O'Day is on a distinguished road
Plaster of Paris is a little different but close, they are both forms of calcium sulfate. There are lots of different plasters and you will need to test the ones you have for what you are doing. Also, I mis-poke about dental plaster, some do not have refractories in them.
Probably the reason pottery plaster started to be used for glass casting is that it is readily available in school studios, not necessarily because it is the best plaster to use. Sometimes the water ratio and mixing is more important than the type of plaster. Consistent testing is important.
Reply With Quote
  #5  
Old 07-13-2019, 11:28 PM
Steven O'Day Steven O'Day is offline
Registered User
 
Join Date: Jun 2002
Location: portland oregon
Posts: 322
Steven O'Day is on a distinguished road
Also, dental plaster investment is often just called dental plaster. Dental plaster is similar to pottery #1 or plaster of Paris, investment is similar to casting mold mix.
Reply With Quote
  #6  
Old 07-14-2019, 12:19 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,956
Franklin Sankar is on a distinguished road
Yes I just discovered there are plaster and there are plaster. Getting the relevant info in the specs. Helps.
Franklin
Reply With Quote
  #7  
Old 07-14-2019, 12:54 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,690
Pete VanderLaan is on a distinguished road
we mix regular plaster with 95 percent alumina castables Franklin. It's nice.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 07-16-2019, 06:52 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,956
Franklin Sankar is on a distinguished road
That sounds like a good use for expired refractory cement. If expired don’t work fresh still is a winner.
Thanks for confirming it’s possible Pete. So it replaces the silica flour.
Franklin
Reply With Quote
  #9  
Old 07-16-2019, 09:08 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,690
Pete VanderLaan is on a distinguished road
It is more refractory than the plaster certainly. It doesn't expand a ton and that's handy. Plaster tends to turn punky when repeat firings are done with it but I think the primary function of the silica is keeping the mold from cracking. Refractory castable does that. I'm not so sure about expired cement.

Missouri Refractory sells calcium aluminate if you ask after it. They never advertise the stuff but it's the cement that makes castables bind and set. I do get 25 lb bags of it and seal it up in airtight containers. Then, when a castable has gone by, I add some. Too much and the peak temperatures for the castable will be compromised.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #10  
Old 07-16-2019, 11:08 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,956
Franklin Sankar is on a distinguished road
Nice how you add the refractory. I am going to try with some green cast 95. Kind of old but itís free. I am most curious to see the outcome. Refractory needs little water but plaster need much more water. That is going to be interesting to see how they work together.
Thanks
Franklin
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 05:43 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.