Cristalica and gaffer

I've been invited to do a couple of demonstrations at a studio that melts Cristalica. Does anyone know how well it will fit with gaffer colours and in particular the duro colours.
Many thanks in anticipation.
Reply With Quote
  #2  
Old 07-28-2019, 11:17 PM
Eric Trulson Eric Trulson is offline
Young Turk
 
Join Date: Sep 2014
Location: Boston
Posts: 119
Eric Trulson is on a distinguished road
It's fine, I've done a bunch of work with cristalica as the base clear glass and gaffer colors. Rod, frit, and duro pulled into cane. Never encountered fit issues at all.
Reply With Quote
  #3  
Old 07-29-2019, 02:08 AM
Peter Bowles Peter Bowles is offline
Registered User
 
Join Date: Sep 2002
Location: Breadalbane, Tasmania
Posts: 634
Peter Bowles is on a distinguished road
Excellent, good to know, thanks Eric
Reply With Quote
  #4  
Old 07-29-2019, 10:07 AM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 600
Art Freas is on a distinguished road
Same here, we haven't had any issues with Gaffer except their blue ice. It worked for a while then something changed and it was very incompatible. Haven't tried it again to see if it was a bad batch.
Reply With Quote
  #5  
Old 07-29-2019, 11:09 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 510
Shawn Everette is on a distinguished road
Ditto on the blue ice. Worked ok as surface frit for pumpkins, but the bar would craze. It's one of their phosphorus opalines, so it's prone to shift compatibility the longer you work it. Other than that I didn't encounter comparability issues.
Reply With Quote
  #6  
Old 07-29-2019, 02:29 PM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 658
Josh Bernbaum is on a distinguished road
Not just the opaline base, but probably the copper shifting things as well in that Blue Ice I'm thinking
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #7  
Old 07-29-2019, 03:14 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,690
Pete VanderLaan is on a distinguished road
copper is really strange stuff. I don't think expansion follows a fixed line of adding it to a batch glass.

I've been mulling over the incompatibility issues some lately. Frank Wooley always asserted ( as did I) that the number of times incompatibility was blamed when it was likely actually poor annealing responsible that I come back to that notion.
In reality, despite my extolling the virtues of making ones own glass is really hard. Attention to detail is critical. Humidity plays hell on calculations. So do scales, so does mixing.

Earlier this year I made a bunch of tumblers and during that period I had a solenoid that keep failing unexpectedly. I'd turn and see the lehr down 400F. I could kick it and bring it back but several loads of these identical opaque cups underwent strain. As time went by, random ones were breaking in differing color combos. They had survived grinding and polishing and sat for quite some time. Some are fine. It just makes me think about annealing and putting work away too cold. Franks claims about that would get Ed Skeels frothing at the mouth.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 07-29-2019, 03:26 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 510
Shawn Everette is on a distinguished road
There's a tech note specifically about the opaline base, don't work it aggressively longer than 30 minutes or the phosphorus with begin to precipitate causing the issues.

It's an interesting pallet of colors, but not interesting enough for me to have to deal with questionable compatibility.
Reply With Quote
  #9  
Old 07-29-2019, 04:58 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,690
Pete VanderLaan is on a distinguished road
A long time ago, Zimmermann made a group of rods called Mother of Pearl. That stuff was gorgeous but it didn't fit whatever we were spewing out at Pilchuck at the time.

I loved Zimmermann. That company had a real connection to a love affair with glass. Of course it failed. Why not?
Anytime you have crystals growing, collapsing and growing again is a Thelma and Louise kind of moment.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #10  
Old 07-29-2019, 05:07 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
rEgisturd Spelunker
 
Join Date: Jan 2007
Location: USSA
Posts: 2,158
Greg Vriethoff is on a distinguished road
I still have some crumbs of Zimmerman floating around. Gonna save it for a special occasion.
__________________
I loves Dale gilhooly
Reply With Quote
  #11  
Old 07-29-2019, 05:45 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,690
Pete VanderLaan is on a distinguished road
I prefer "Technique is a way of finding out you can make a statement."
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #12  
Old 07-29-2019, 06:50 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 958
Larry Cazes is on a distinguished road
Quote:
Originally Posted by Shawn Everette View Post
There's a tech note specifically about the opaline base, don't work it aggressively longer than 30 minutes or the phosphorus with begin to precipitate causing the issues.

It's an interesting pallet of colors, but not interesting enough for me to have to deal with questionable compatibility.
When it first was released I had horrendous problems with Gaffer Alabaster. Gave up on it and haven't tried it since but I really loved the translucent qualities. I would garage the rod around 950 and usually put two lengths in for good measure. No problems working it but all of the spare unworked rods came out after annealing completely spider webbed with cracks and unusable. Never happened with any other colors.
Reply With Quote
  #13  
Old 07-29-2019, 07:23 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 510
Shawn Everette is on a distinguished road
Yeah, they say it's no good if left in the color box all day too. Seems like frit or quick rod work are the only way to go with it, which kind of makes it not exactly the most useful.
Reply With Quote
  #14  
Old 07-29-2019, 08:48 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 600
Art Freas is on a distinguished road
Quote:
Originally Posted by Shawn Everette View Post
Ditto on the blue ice. Worked ok as surface frit for pumpkins, but the bar would craze. It's one of their phosphorus opalines, so it's prone to shift compatibility the longer you work it. Other than that I didn't encounter comparability issues.
We had issues with Frit when it was encased as well. All the variables were the same except the batch of blue ice. Stuff would look great out of the annealer and then day by day more an more cracks.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 05:32 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.