Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,690
Pete VanderLaan is on a distinguished road
As always, Dudley's gizmos provide endless entertainment. It's such a rat's nest! Anyone who hasn't visited his barn should do it.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 07-16-2019, 06:58 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,956
Franklin Sankar is on a distinguished road
I bet your Barn is more interesting. No we don’t have barns. Cow sheds yes.
I wish Dudley would make more low pressure stuff.
Franklin
Reply With Quote
  #4  
Old 07-16-2019, 09:10 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,611
Eben Horton is on a distinguished road
Very cool.
I made glass with Dudley in the late 90ís and learned a few cool tricks. Especially how to pull bead stock.
__________________
<eben epoiese>
Reply With Quote
  #5  
Old 07-16-2019, 09:11 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,690
Pete VanderLaan is on a distinguished road
No, Dudley's is more interesting. He's big on high pressure so he doesn't have to use blowers. All propane tanks can output high pressure and it's part of the philosophy of not wanting inspectors around since they rarely have imaginations. Dudley has quite a good one.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 05:55 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.