Looking for some advice and suggestions. I have some wooden display shelving acting as a wall / gallery space behind my annealers. I feel like I should attach something to the back of the wooden shelving unit to protect it from the annealers radiant heat. The annealer don't really put out much external heat but figured prevention from problems is best. Even if it's really about appearances for building official's. The large annealer is about 6-8" away from the shelving. I was thinking drywall (although it's heavy and I drive a small SUV) or maybe that reflective foam board. Anyone have any input? Thanks again for any help
Reply With Quote
  #2  
Old 07-07-2019, 04:55 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 230
Shawn Everette is on a distinguished road
Hardiebacker, ugly but works.
Reply With Quote
  #3  
Old 07-07-2019, 05:30 PM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,507
Eben Horton is on a distinguished road
Id use galvanized sheet metal
__________________
<eben epoiese>
Reply With Quote
  #4  
Old 07-07-2019, 06:11 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,102
Pete VanderLaan is on a distinguished road
multiple dead air spaces.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 07-07-2019, 06:11 PM
Philip Yamron Philip Yamron is offline
Registered User
 
Join Date: Jul 2012
Location: Ann Arbor, MI
Posts: 76
Philip Yamron is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
multiple dead air spaces.
Could you elaborate please
Reply With Quote
  #6  
Old 07-07-2019, 07:52 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,102
Pete VanderLaan is on a distinguished road
Dead air is the best insulator. When I built my hood I laid in multiple layers of sheet rock with spacing in between each layer.

In your case, I would put some spacers on the portion of the shelving facing the lehr about an inch thick and would attach a piece of aluminized foam. Then another set of spacers, then a piece of sheet rock, then a set of spacers and a last piece of rock.The aluminized stuff really insulates but the resin in the foam is actually flammable so it goes up furthest away from the heat. To see how well this might work, set up a similar arrangement somewhere nearer the front of the lehr where you can mess with it and change the arrangement if you're unhappy with it. Stick a thermocouple where you can get a reading back in the place the shelves would be when doing the real thing.

I used to think that 160F was acceptable as an ambient temp for radiant heat but years of studing studio fires as well as pyrolytic fires when I ran the fire dept taught me that was was too high. These days 130-135 makes me comfortable.

Materials don't burn, the gas vapor coming off of them does. Gradually as materials decompose over the years, they're far more prone to gassing. I have seen fires go through concrete slabs 10 inches thick and fireplace outgasses were constant. Here in New England, Chimney fires are the main problem which we rarely had out west. They all involve cracked flue tile, just again and again. Stainless flexible pipe solves the bulk of that problem.

So shoot for those temps. The trouble with simply using rock, or whatever is that the heat eventually passes through it to the other side and comes to stasis. While asbestos doesn't in fact burn, it's really useless. Let it breathe.

Do I need to say more or is it clear?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 07-08-2019, 03:12 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 942
Sky Campbell is on a distinguished road
Cheap metal 2x4s and corrugated tin roofing. Would be my go to.
Reply With Quote
  #8  
Old 07-08-2019, 08:16 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,102
Pete VanderLaan is on a distinguished road
whatever gives you dead air space.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #9  
Old 07-10-2019, 07:11 PM
Philip Yamron Philip Yamron is offline
Registered User
 
Join Date: Jul 2012
Location: Ann Arbor, MI
Posts: 76
Philip Yamron is on a distinguished road
Thanks everyone. I deeply appreciate the help this forum/community offers.

Philip
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 06:38 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.