Annealing schedule for crystalica

I bit the bullet and bought a tonne of crystalica but donít have an annealing schedule for overnight. They havenít published one and canít help as their technical bod is on holiday. The website has one for 1 inch thick but I need an overnight schedule for stemware.
Iíve built a 3 cubic foot box with 3Ē of fibre the runs great at 3kW through an SCR but would cool too slowly if I just turned it off.
Iíve got Glass Notes 4 and can use that but it seems mad to have to calculate it. Can anyone help.
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 11:06 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.